The high-strength structural steel at 650-700 MPa

Strenx™ 700 E/F is a structural steel with a minimum yield strength of 650-700 MPa depending on thickness.

Strenx™ 700 E/F meets the requirements of EN 10 025-6 for the S690 grade and thicknesses. Typical applications include demanding load-bearing structures.

Strenx™ 700 E (complies with S690QL) is available in plate thicknesses of 4–160 mm, while Strenx™ 700 F (complies with S690QL1) is available in plate thicknesses of 4–130 mm.

Benefits include:

  • Superior bendability and surface quality
  • Weldability with excellent HAZ strength and toughness
  • Exceptional consistency within a plate guaranteed by close tolerances
  • High impact toughness which provides for good resistance to fractures

Dimension Range

Strenx® 700 E is available as plate in thicknesses of 4.0 – 160.0 mm and Strenx® 700 F is available as plate in thicknesses of 4.0 - 130.0 mm. Both grades are available in widths up to 3350 mm and lengths up to 14630 mm depending on thickness. More detailed information on dimensions is provided in the dimension program.

Available Standards

EN 10025-6

EN 10029

EN 10163-2

Strenx® 700 E/F

Strenx® 700 E/F

USED FOR
DIMENSIONS
STANDARDS
DATA SHEET
USED FOR

Structural

Low temperatures (down to -60°)

DIMENSIONS

T: 0.16 - 6.3 Inches

W: Up to 131.89 Inches

L: Up to 575.98 Inches

STANDARDS

EN 10025-6

EN 10029

EN 10163-2