Strenx™ 700 CR
The high-strength structural steel at 700 MPa
Strenx™ 700 CR is a cold-rolled structural steel with a minimum yield strength of 700 MPa used to produce stronger and lighter structures.
Strenx™ 700 CR comes in cut-to-length sheets. Typical applications include a wide range of components and parts, for example load-bearing structures.