SSAB Domex® 280LA is a high-strength, low-alloy steel intended for general presswork, bending and forming. Typical applications include bent profiles.

SSAB Domex® 280LA offers consistent properties that assist modern, rapid production methods.

SSAB Domex 280LA is available in thicknesses of 0.40-3.00 mm and widths up to 1500 mm as coils, slit coils and as cut to length in lengths up to 8.5 meters.

Available Standards

EN 10131

SSAB Domex 280LA

SSAB Domex 280LA

USED FOR
DIMENSIONS
STANDARDS
DATA SHEET
USED FOR

Structural

DIMENSIONS

T: 0.02 - 0.12 Inches

W: Up to 59.06 Inches

L: Up to 334.65 Inches

STANDARDS

EN 10131