Hardox 600
Hardox 600 - Extra hard and tough steel for extreme wear

Hardox® 600

The extra hard and tough steel for extreme wear

At a nominal hardness of 600 HBW, Hardox® 600 has a uniquely high impact toughness.

Especially suited for extreme wear conditions, it can still be cut and welded, making it an excellent choice for high-performance applications.

 

Order trial material Get free technical advice

What is hardness?

Hardox wear steel for extreme abrasion resistance

Dimension Range

Hardox® 600 is available as plate in thicknesses of 6.0 – 65.0 mm and as sheet in thicknesses of 3.0 - 6.0 mm. Hardox® 600 is available in widths up to 2000 mm and lengths up to 14630 mm. Preferred dimensions for the plates are 2000 x 4000 mm and for the sheets the preferred dimensions are 1250 x 3000 or 1500 x 3000 mm depending on thickness. Other dimensions on request. More detailed information on dimensions is provided in the dimension program.

 

Available Standards

EN 10029

EN 10051

Hardox® 600

Hardox® 600

USED FOR
DIMENSIONS
STANDARDS
DATA SHEET
USED FOR

Wear Resistant

DIMENSIONS

T: 0.12 - 2.56 Inches

W: Up to 78.74 Inches

L: Up to 575.98 Inches

STANDARDS

EN 10029

EN 10051

DATA SHEET