GreenCoat Pro BT
Proven durability that outlasts the harshest weather.
GreenCoat Pro BT color coated steel is available in regular and matt finishes and offers a wide range of colors inspired by Nordic nature. It uses a patented bio-based coating having Swedish rapeseed oil instead of traditional fossil oil in the paint, which is unique on the market. SSAB holds a worldwide patent for this coating technology (Bio-based Technology, BT).
GreenCoat Pro BT is highly durable and has mainly been developed for roofing applications like profiled roof tiles or standing seam systems. For tinsmith applications, GreenCoat PLX Pro BT and the FAP steel grade offered with GreenCoat Pro BT is additionally available. GreenCoat Pro BT possesses excellent forming properties enabling very demanding folding even down to -15°C, allowing for year round installation at lower costs.
GreenCoat Pro BT color coated steel is also optimized for wear resistance, weathering resistance and low resource consumption. It has greater durability than standard polyester products when exposed to people walking on the roof and other roof stresses. The product possesses excellent gloss retention and color fastness. It also provides good protection against corrosion reaching the highest RC5+ class.
The reverse side of the sheet is painted with a two-layer grey backside coating.
GreenCoat Pro BT complies with current REACH regulations and is fully free of chromates.