ABS Grade EQ51

Download data sheet

General Product Description

Our ABS Grades EQ51 is a high-strength, thermo-mechanically controlled rolled structural steel having a minimum specified yield strength of 73 ksi and specified minimum Charpy V-notch impact toughness properties.

Applications

Typical applications include shipbuilding and mobile offshore drilling units and structures.

Available Dimensions

Grade
Grade
Grade EQ51
Product type
Plate
Thickness
(in)
0.393 - 1.57
Width
(in)
75 - 129.9
Length
(in)
79 - 590

Mechanical Properties

Grade
Grade
Grade EQ51
Thickness
(in)
0.393 - 1.57
0.2% YS
(ksi)
73
UTS
(ksi)
88 - 112
Elongation A5 1)
(min %)
16

1) See ABS Rules for elongation requirements for alternative tensile specimens.

Impact Properties

Grade
Grade
Grade EQ51
Thickness
(in)
0.393 - 1.57
Test temperature
(°F)
-40
Min Longitudinal Average Energy 1)
(ft-lbs)
37
Min transverse average energy 1)
(ft-lbs)
24

1) Specimen orientation at the option of the manufacturer unless otherwise specified in the order.

No more than one value below the specified miniminum average energy but no less than 70% of the specfied minimum average energy value.

Minimum average energy for full-size specimens. Refer to ABS Rules for sub-size specimen energy requirements.