Hardox® HiTemp

The Hardox® wear plate that can take the heat

Hardox® HiTemp is a high-heat grade of Hardox® wear plate that provides a cost-efficient solution for wear resistance at high temperatures in the 300–500°C range (570–930°F).

Whereas traditional quenched and tempered wear-resistant steels lose hardness at higher temperatures, Hardox® HiTemp high-temperature steel delivers extreme wear resistance. Its properties are achieved by using high-quality raw material combined with a carefully controlled manufacturing process.

Hardox® HiTemp is delivered as 5–51 mm (0.197’’–2’’) plate. It can be cut, welded and machined using the same kind of machinery and technology as for conventional steel.

Order trial material I'm interested, contact me

Prezentare a noului oțel Hardox® HiTemp

Dimension Range

Hardox® HiTemp is available as plate in thicknesses of 4.7 – 51.0 mm. Hardox® HiTemp is  available in widths up to 3350 mm and lengths up to 14630 mm. More detailed information on dimensions is provided in the dimension program.

 

Available Standards

EN 10029

EN 10163-2

Hardox® HiTemp

Hardox® HiTemp

UTILIZARE
DIMENSIUNI
STANDARDE
FIȘĂ TEHNICĂ
UTILIZARE

Wear Resistant

DIMENSIUNI

T: 4.7 - 51 mm

W: Up to 3350 mm

L: Up to 14630 mm

STANDARDE

EN 10029

EN 10163-2

FIȘĂ TEHNICĂ