SSAB M53
Download data sheet
Download data sheet
Delivery form | Thickness (mmin) |
Width (mmin) |
Max. length (mmin) |
---|---|---|---|
Hot rolled sheet | 4.0 - 8.0 1)0.16 - 0.31 1) | 1000 - 180039.37 - 70.87 | 13000511.81 |
1) Please check thickness/width combinations available.
Product type | Typical yield strength (MPa), not guaranteed |
Typical tensile strength Rm (MPa), not guaranteed | Typical Elongation A (%),not guaranteed | Typical Hardness (HRC), not guaranteed |
---|---|---|---|---|
As rolled | 460 - 700 | 700 - 1000 | 14 | 15 - 32 |
Polymer quenched | — | — | — | 60 - 63 |
Polymer quenched & tempered (175° C) | — | — | — | 59 - 61 |
Polymer quenched & tempered (425° C) | 1400 | 1500 | 8.5 | 47 |
Polymer quenched & tempered (550° C) | 1180 | 1270 | 11.5 | 42 |
Oil quenched | — | — | — | 59 - 61 |
Oil quenched and tempered (175° C) | — | — | — | 59 - 61 |
Oil quenched and tempered (425° C) | 1440 | 1550 | 8.5 | 48 |
Oil quenched and tempered (550° C) | 1210 | 1290 | 11.5 | 43 |
Examples of cooling media used for evaluating typical mechanical properties:
PAG polymer 10%, no agitation, T ≤ 30 °C.
Fast cooling rate quenching oil, T ≤ 35 °C.
For further information, please consult your local SSAB contact person or contact SSAB´s Technical Customer Service.
A material test certificate Type 2.2 according to EN 10204 (chemical composition) is part of the delivery.
A material test certificate according Type 3.1 according to EN 10204 (mechanical properties) can be provided by special agreement.
Product condition | Longitudinal test, typical impact energy, Charpy V 10x10 mm test specimen 1) |
---|---|
As rolled | — |
Polymer quenched | 9 J / 20.0 °C |
Polymer quenched & tempered (175° C) | 18 J / 20.0 °C |
Polymer quenched & tempered (425° C) | 26 J / 20.0 °C |
Polymer quenched & tempered (550° C) | 41 J / 20.0 °C |
Oil quenched | 9 J / 20.0 °C |
Oil quenched and tempered (175° C) | 18 J / 20.0 °C |
Oil quenched and tempered (425° C) | 24 J / 20.0 °C |
Oil quenched and tempered (550° C) | 40 J / 20.0 °C |
1) For thicknesses between 6 - 11.9 mm, sub-size Charpy V-specimens are used. The specified typical value is then proportrional to the cross-sectional area of the specimen compared to a full-size specimen (10 x 10 mm).
Delivery form | C (%) |
Si (%) |
Mn (%) |
S (max %) |
P (max %) |
Cr (max %) |
---|---|---|---|---|---|---|
Hot rolled strip | 0.49 - 0.57 | 0.10 - 0.35 | 0.15 - 0.50 | 0.010 | 0.020 | 0.60 |
SSAB M53 is micro-alloyed with Nb, Ti and V.
Delivery form | Hot rolled strip |
---|---|
Typical CET (%) | 0.61 |
SSAB M53 is delivered with SSAB tolerances, which meet and exceed the requirements in EN 10051. Tighter tolerances are available upon request
2/3 of EN 10051.
Hot rolled sheet: -0/+20mm.
Tolerances according to EN 10051.
≤ 6 mm/1 m ruler deviation (only valid for cut to length sheets).
According to EN 10163-2 Class A, Subclass 3.
Hot rolled sheet are delivered in as rolled (+AR) condition.
Hot rolled strip products are available in non-pickled.
Pickled dry or pickled & oiled condition available upon request.
Cutting is recommended by laser or plasma, flame cutting is not advised.
For information concerning fabrication, see SSAB´s brochures on www.ssab.com or consult Tech Support.