Rough Matt Polyester

Download data sheet

Select Language

Get datasheet by email
Close

Get datasheet by email

    General Product Description

    Rough Matt Polyester color coated steel from SSAB is available in a rough matt finish and offers colors inspired by Nordic nature. 

    It has specifically been developed for the use in tiles and other roofing profiles and offers good profiling properties which are reached through a harder surface resulting in a product which is “problem-free” during profiling, transportation and installation. The long-term durability properties are according to SSAB’s high standards.

    The reverse side of the sheet is painted with a two-layer grey backside coating.
     
    Rough Matt Polyester complies with current REACH regulations and is fully free of chromates.

    SSAB’s color coated steels are all manufactured according to EN 10169.

    Technical Properties

    Hide/Show specific columns Edit
    Select columns to display
      Technical Properties
      Gloss 4
      Minimum inner bending radius 2 x sheet thickness
      Scratch resistance 25 N
      UV radiation resistance RUV3
      Corrosion resistance 1) RC4
      Stain resistance Good
      Highest operating temperature 90 °C
      Fire classification, EN 13501-1 A2 s1 d0
      Coating thickness, nominal (primer + top coat) 30 µm
      Coating structure Structured
      Steel designation 2) S280GD, S320GD, S350GD
      Zinc coating 275 g/m2
      Min steel thickness 2) 0.45 mm
      Steel width 2) 1000 - 1300 mm
      Compare parameters

      Select one parameter to compare

      Comparison

        Technical Properties
        Gloss
        4
        Technical Properties
        Minimum inner bending radius
        2 x sheet thickness
        Technical Properties
        Scratch resistance
        25 N
        Technical Properties
        UV radiation resistance
        RUV3
        Technical Properties
        Corrosion resistance 1)
        RC4
        Technical Properties
        Stain resistance
        Good
        Technical Properties
        Highest operating temperature
        90 °C
        Technical Properties
        Fire classification, EN 13501-1
        A2 s1 d0
        Technical Properties
        Coating thickness, nominal (primer + top coat)
        30 µm
        Technical Properties
        Coating structure
        Structured
        Technical Properties
        Steel designation 2)
        S280GD, S320GD, S350GD
        Technical Properties
        Zinc coating
        275 g/m2
        Technical Properties
        Min steel thickness 2)
        0.45 mm
        Technical Properties
        Steel width 2)
        1000 - 1300 mm

        1) Classification into corrosion resistance categories is based on blistering, delamination and damage on bend of the coating after two years exposure in natural outdoor testing sites as specified in EN 10169.

        2) Maximum steel thickness is 1.5 mm and maximum steel width depends on steel thickness. For other steel dimensions or steel grades please contact SSAB Tech Support.

        Colors

        Below are the colors currently available. Other colors can be agreed upon separately.

        Colors shown in the color table are only indicative. To see the real visual appearance of the product, please order a color sample. Please note also that the same colors between the products may differ.

        8 Available Colors
        Preview colors
        Close

        Colors

        Rough Matt Polyester

        Mountain Grey

        RR23 / SS0036

         

        Slate Grey

        RR2H3 / SS0534

         

        Nordic Night Black

        RR33 / SS0015

         

        Walnut Brown

        RR32 / SS0387

         

        Chestnut Brown

        RR887 / SS0435

         

        Cottage Red

        RR29 / SS0758

         

        Tile Red

        RR750 / SS0760

         

        Pine Green

        RR11 / SS0830

         

        Note for all colors: To ensure tonal consistency of colors on a single exterior face, all material must come from the same production batch. Also the directionality of surfaces has to be consistent especially when sheets are cut to size.

        Reverse Side Coating

        Unless otherwise specified, the reverse side of the sheet is painted with a two-layer coating to further improve the corrosion resistance of the end product. The coating provides good adhesion properties to many adhesives and foams; nevertheless the compatibility needs to be tested case-specifically.

        Hide/Show specific columns Edit
        Select columns to display
          Technical Properties
          Nominal Coating Thickness (primer + top coat) 12 µm
          Color Grey
          Corrosion Resistance Min CPI3
          Compare parameters

          Select one parameter to compare

          Comparison

            Technical Properties
            Nominal Coating Thickness (primer + top coat)
            12 µm
            Technical Properties
            Color
            Grey
            Technical Properties
            Corrosion Resistance
            Min CPI3

            For easy material identification the reverse side of the sheet is stamped with the SSAB logo and the product name. The production year is marked to ease material traceability and can be referred to within the guarantee period. An arrow shows the direction of production to ensure installation in a uniform direction.