GreenCoat Pural BT

Download data sheet

Select Language

Get datasheet by email
Close

Get datasheet by email

    General Product Description

    GreenCoat Pural BT color coated steel is available in regular and matt finishes and offers a wide range of colors inspired by Nordic nature. It uses a patented bio-based coating having Swedish rapeseed oil instead of traditional fossil oil in the paint, which is unique on the market. SSAB holds a worldwide patent for this coating technology (Bio-based Technology, BT).

    GreenCoat Pural BT offers the highest level of durability for roofing applications like standing seams, profiled roof tiles and is used widely in metal roofer applications. Besides the regular gloss GreenCoat Pural BT in non-metallic colors can be used in facade products like, sandwich panels and cassettes.

    GreenCoat Pural BT color coated steel offers a coating that is optimized to resist weathering resulting in the highest UV (Ruv5 for matt appearance) and corrosion classes (RC5+). The slightly structured surface helps to protect against mechanical wear and is easy to handle during manufacturing. GreenCoat Pural BT possesses excellent forming properties enabling very demanding folding even down to -15°C, allowing for year round installation at lower costs.

    The reverse side of the sheet is painted with a two-layer grey backside coating.

    GreenCoat Pural BT complies with current REACH regulations and is fully chromate-free.

    SSAB’s color coated steels are all manufactured according to EN 10169.

    GreenCoat and Pural are trademarks of the SSAB group of companies.

    Technical Properties

    Hide/Show specific columns Edit
    Select columns to display
      Technical Properties Matt Regular
      Gloss < 5 40
      Minimum inner bending radius 1 x sheet thickness 1 x sheet thickness
      Scratch resistance 40 N 40 N
      Lowest forming temperature -15 °C -15 °C
      UV radiation resistance RUV5 RUV4
      Corrosion resistance 1) RC5+ RC5+
      Stain resistance Very good Very good
      Highest operating temperature 100 °C 100 °C
      Fire classification, EN 13501-1 A1 s1 d0 A1 s1 d0
      Coating thickness, nominal (primer + top coat) 50 µm 50 µm
      Coating structure Structured Structured
      Steel designation 2) S280GD, S320GD, S350GD S280GD, S320GD, S350GD
      Zinc coating 275 g/m2 275 g/m2
      Min steel thickness 2) 0.50 mm 0.50 mm
      Steel width 2) 1000 - 1500 mm 1000 - 1500 mm
      Compare parameters

      Select one parameter to compare

      Comparison

        1) Classification into corrosion resistance categories is based on blistering, delamination and damage on bend of the coating after four years exposure in natural outdoor testing sites as specified in EN 10169.

        2) Maximum steel thickness is 1.5 mm and maximum steel width depends on steel thickness. For other steel dimensions or steel grades please contact SSAB Tech Support.

        Colors

        Below are the colors currently available. Other colors can be agreed upon separately.

        Colors shown in the color table are only indicative. To see the real visual appearance of the product, please order a color sample. Please note also that the same colors between the products may differ.

        For information on thermal properties (solar reflectance index SRI or thermal emittance TE) of available colors, please contact SSAB Tech Support.

        30 Available Colors
        Preview colors
        Close

        Colors

        GreenCoat Pural BT

        Winter White

        RR20 / SS0005

        Regular, Matt

        Snow White

        RR19 / SS0001

        Matt

        Concrete Grey

        RR292 / SS----

        Regular

        Pebble Grey

        RR21 / SS0011

        Regular, Matt

        Quarry Grey

        RR287 / SS0244

        Regular, Matt

        Stone Grey

        RR22 / SS0554

        Regular, Matt

        Rock Grey

        RR237 / SS0061

        Regular

        Anthracite Grey

        RR2H8 / SS0087

        Matt

        Mountain Grey

        RR23 / SS0036

        Regular, Matt

        Ridge Grey

        RR2F7 / SS0035

        Regular

        Slate Grey

        RR2H3 / SS0534

        Regular, Matt

        Nordic Night Black

        RR33 / SS0015

        Regular, Matt

        Walnut Brown

        RR32 / SS0387

        Regular, Matt

        Chestnut Brown

        RR887 / SS0435

        Regular, Matt

        Almond Brown

        RR30 / SS0187

        Regular

        Terra Brown

        RR31 / SS0433

        Regular

        Cottage Red

        RR29 / SS0758

        Regular, Matt

        Tile Red

        RR750 / SS0760

        Regular, Matt

        Brick Red

        RR7F2 / SS0742

        Regular

        Wine Red

        RR798 / SS5781

        Regular, Matt

        Harvest Yellow

        RR24 / SS0189

        Regular

        Silver Fir Green

        RR5J3 / SS0975

        Matt

        Leaf Green

        RR594 / SS0874

        Matt

        Pine Green

        RR11 / SS0830

        Regular, Matt

        Green

        RR37 / SS0925

        Regular

        Lake Blue

        RR35 / SS0558

        Regular

        Metallic Silver

        RR40 / SS0045

        Regular

        Metallic Dark Silver

        RR41 / SS0044

        Regular, Matt

        Metallic Gold

        RR974 / SS0645

        Regular

        Metallic Copper

        RR979 / SS0778

        Regular

        Note especially for Metallic and all Matt colors: To ensure tonal consistency of colors on a single exterior face, all material must come from the same production batch. Also the directionality of surfaces has to be consistent especially when sheets are cut to size. Compared to solid colors, larger measured color variation between production batches is typical for metallic colors, even if color is visually stable.

        Reverse Side Coating

        Unless otherwise specified, the reverse side of the sheet is painted with a two-layer coating to further improve the corrosion resistance of the end product. The coating provides good adhesion properties to many adhesives and foams; nevertheless the compatibility needs to be tested case-specifically.

        Hide/Show specific columns Edit
        Select columns to display
          Technical Properties
          Nominal Coating Thickness (primer + top coat) 12 µm
          Color Grey
          Corrosion Resistance Min CPI3
          Compare parameters

          Select one parameter to compare

          Comparison

            Technical Properties
            Nominal Coating Thickness (primer + top coat)
            12 µm
            Technical Properties
            Color
            Grey
            Technical Properties
            Corrosion Resistance
            Min CPI3

            For easy material identification the reverse side of the sheet is stamped with the GreenCoat logo and the product name. The production year is marked to ease material traceability and can be referred to within the guarantee period. An arrow shows the direction of production to ensure installation in a uniform direction.

            Contact Information

            www.ssab.com/contact