Epoxy

Download data sheet

Select Language

Get datasheet by email
Close

Get datasheet by email

On this page

General Product Description

Epoxy color coated steel from SSAB is available in regular and matt finishes. It is used in different indoor building applications, but also in other industries like inside walls for passenger buses. 

Epoxy color coated steel is well suited for objects that are later finished with the color chosen by the customer. It can also be used in indoor applications where wallboards or tiles are bonded on the surface. Light washing is enough as a pre-treatment. 

Epoxy color coated steel offers good adhesion and corrosion resistance.

The reverse side of the sheet is painted with a two-layer grey backside coating.

Epoxy complies with current REACH regulations and is fully free of chromates.

SSAB’s color coated steels are all manufactured according to EN 10169.

Technical Properties

Hide/Show specific columns Edit
Select columns to display
    Technical Properties Regular Matt
    Gloss 35 10
    Minimum inner bending radius 5 x sheet thickness 5 x sheet thickness
    Corrosion resistance Min CPI3 Min CPI3
    Highest operating temperature 110 °C 110 °C
    Coating thickness, nominal (primer + top coat) 12 µm 12 µm
    Compare parameters

    Select one parameter to compare

    Comparison

      Colors

      Epoxy is available in standard grey (reverse side color). Other colors can be agreed upon separately.

      1 Available Colors
      Preview colors
      Close

      Colors

      Epoxy

      Grey

      RR18 / SS0012

      Regular, Matt

      Reverse Side Coating

      Hide/Show specific columns Edit
      Select columns to display
        Technical Properties
        Nominal Coating Thickness (primer + top coat) 12 µm
        Color Grey
        Corrosion Resistance Min CPI3
        Compare parameters

        Select one parameter to compare

        Comparison

          Technical Properties
          Nominal Coating Thickness (primer + top coat)
          12 µm
          Technical Properties
          Color
          Grey
          Technical Properties
          Corrosion Resistance
          Min CPI3

          Contact Information