Duroxite® AP Wire

Download data sheet

Select Language

Get datasheet by email
Close

Get datasheet by email

    Descrierea generală a produsului

    Duroxite® AP Wire is a gas shielded flux cored all positions hardfacing wire for components experiencing metal-to-metal wear, metal-to-earth wear, impact and high abrasion applications. The deposit offers a good balance of impact and abrasion resistance. Deposits are forgeable but not readily machinable. The wire has been developed to operate in a smooth semi-spray transfer mode whilst welding in all positions. Duroxite®  AP Wire can be applied to carbon, low alloy, ,manganese and other steels substrates. The deposited overlay is magnetic on carbon and low alloy steels but not on manganese steels. Duroxite® AP Wire is suitable for single and multiple-layer up to three layers deposit.

    Key Benefits

    • Duroxite® AP Wire is a hardfacing wire for all positions welding.
    • The Duroxite® AP WIRE deposited overlay consists of medium alloy martensite for good abrasion and impact resistance.

    Typical Applications

    Duroxite® AP Wire has many applications where moderate/high impact and high abrasion wear conditions prevail. Examples: Bucket teeth, tillage tools, bucket lips, bucket sides, cutting edges, sand dredge equipment, dragline buckets, conveyor chutes, grizzly bars, screw flights, metal shredders, sliding metal parts, tire shredder knives, extruder screws, tamper feet, churn drills, muller tires. Especially applicable for all-positional welding and re-instating of hardfacing sealing runs on clad wear plate fabrications.

    Standard Dimensions

    Hide/Show specific columns Edit
    Select columns to display
      Standard diameter
      Metric
      1.6 mm
      Compare parameters

      Select one parameter to compare

      Comparison

        Standard diameter
        Metric
        1.6 mm

        Proprietăți mecanice

        Hide/Show specific columns Edit
        Select columns to display
          Typical all-weld metal surface Hardness 1)
          Hardness: 2-layer deposit on mild steel Hardness: 3-layer deposit on mild steel
          55 - 59 HRC 56 - 60 HRC
          Compare parameters

          Select one parameter to compare

          Comparison

            Typical all-weld metal surface Hardness 1)

            Hardness: 2-layer deposit on mild steel
            55 - 59 HRC
            Typical all-weld metal surface Hardness 1)

            Hardness: 3-layer deposit on mild steel
            56 - 60 HRC
            1) Surface hardness is measured on machined flat surface just below overlay surface.

            Chemical Composition

            Hide/Show specific columns Edit
            Select columns to display
              Typical all-weld metal analysis (Weight %)
              C
              (%)
              Mn
              (%)
              Si
              (%)
              Cr
              (%)
              Mo
              (%)
              Fe
              0.5 1.3 Up to 0.6 7.0 0.6 Balance
              Compare parameters

              Select one parameter to compare

              Comparison

                Welding recommendations

                Hide/Show specific columns Edit
                Select columns to display
                  Welding conditions
                  Current type Shielding gas Welding positions
                  DCEP (Direct current electrode positive) 75% Ar + 25% CO2 gas mixtures All Positions including flat, horizontal, vertical, overhead
                  Compare parameters

                  Select one parameter to compare

                  Comparison

                    Welding parameters recommendations

                    Hide/Show specific columns Edit
                    Select columns to display
                      Diameter
                      Amperage (A)
                      Voltage (V)
                      Stick-out
                      Metric Range Optimum Range Optimum Range Optimum
                      1.6 mm 170 - 275 220 24 - 30 28 12 mm - 30 mm 20 mm
                      Compare parameters

                      Select one parameter to compare

                      Comparison

                        Recovery: 90%

                        Condiții de livrare

                        Hide/Show specific columns Edit
                        Select columns to display
                          Standard package
                          Weight
                          Type
                          Spool 15
                          Compare parameters

                          Select one parameter to compare

                          Comparison

                            Standard package
                            Type
                            Spool
                            Weight
                            15

                            Fabricare și alte recomandări

                            The welded overlay components can be processed by welding, cutting, forming and machining. Specific recommendations can be found in the Duroxite® Product brochure or by consulting your local technical support representative.

                            Safety precautions

                            When welding or cutting Duroxite® products, smoke is produced containing harmful fumes and gases that are chemically highly complex and difficult to easily classify. The major toxic component in the fumes and gases produced in the process is hexavalent chromium. The proper exhaust ventilation equipment and fume-extraction torches are recommended, as well as suitable protective clothing and respiratory protection for operators.