    Descrierea generală a produsului

    Duroxite® 100 Pipe is manufactured by depositing chromium-rich, abrasion-resistant materials on a mild steel base using a traditional arc welding process. The hardfacing overlay pipe is designed with extreme wear capabilities for working in the most severe environments. Duroxite® 100 Pipe is available with double or multiple overlay passes. Schedule 40 and Schedule 80 steel pipe as well as tubing can be hardfaced. Overlay Pipe can be fabricated as square-to-round transitions, elbows, T or Y-shaped, or as long sweeps.

    Key Benefits

    • Same wear resistance guaranteed from surface down to 75% of the overlay
    • Optimal carbide composition to provide good combination of wear resistance and homogenous bonding

    Typical Applications

    Duroxite® 100 Pipe is widely used in the mining, cement, oil sands, dredging, recycling and steel production industries. Some specific applications include:

    Hide/Show specific columns Edit
    Select columns to display
      Mining, Cement, Oil Sands Slurry pumps, chutes
      Dredging Dredging pipes
      Recycling Cullet glass
      Steel Air ducts, carbon injection pipes, suction lines, troughs
      Compare parameters

      Select one parameter to compare

      Comparison

        Mining, Cement, Oil Sands
        Slurry pumps, chutes
        Dredging
        Dredging pipes
        Recycling
        Cullet glass
        Steel
        Air ducts, carbon injection pipes, suction lines, troughs

        For more information on applications see the Duroxite® Product brochure.

        Standard Dimensions

        Hide/Show specific columns Edit
        Select columns to display
          Diameter
          Length
          Metric unit Metric unit Other Custom Specifications
          150 mm
          175 - 350 mm
          375 - 600 mm
          625 - 900 mm
          1.0 m
          0.9 - 3.0 m
          0.9 - 6.0 m
          1.8 - 6.0 m
          - All available gauges > Schedule 40 steel pipe
          - Lengths cut or fabricated as needed
          - Stainless steel and other pipe grades available
          - Custom diameter lengths and gauge sizes are available upon request
          - Diameters larger than 36” can be fabricated from formed Duroxite® 100 plate
          Compare parameters

          Select one parameter to compare

          Comparison

            Other plate sizes and custom thicknesses can be produced upon request.

            Proprietăți mecanice

            Hide/Show specific columns Edit
            Select columns to display
              Wear properties
              ASTM G65 – Procedure A weight loss 2)
              Number of overlay passes Typical surface hardness1)

              (HRC)
              Typical surface hardness1)

              (HV)
              Surface
              (g max)
              75 % depth of overlay 3)
              (g max)
              Double or multiple 59 - 62 675 - 750 0.18 0.18
              Compare parameters

              Select one parameter to compare

              Comparison

                1) Surface hardness is measured on machined flat surface just below overlay surface.

                2) ASTM G65 - Procedure A weight loss, is a standard test measuring sliding abrasion resistance using a dry sand/rubber wheel apparatus. ASTM G65-Procedure A is the most severe test method.

                3) ASTM G65 - Procedure A weight loss, wear test is conducted at 75% depth of the overlay materials to ensure consistently good wear resistance from the top surface through to the depth of 75% of the overlay.

                Microstructure

                The microstructure of Duroxite® 100 Pipe is composed of a high proportion of extremely hard primary M7C3 chromium-rich carbides with a typical hardness of 1700 HK4) dispersed evenly in a ductile eutectic austenite matrix. The volume fraction of primary carbides is maintained between 30 to 50% to provide a good combination of wear resistance and homogenous bonding.

                4) HK is the Knoop microhardness used primarily for very brittle materials.

                Fabricare și alte recomandări

                Welding, cutting, forming and machining

                Workshop recommendations can be found in the Duroxite® overlay brochure or you can consult your local technical support representative for more information.

                Safety precautions

                When welding or cutting Duroxite® products, smoke is produced containing harmful fumes and gases that are chemically highly complex and difficult to easily classify. The major toxic component in the fumes and gases produced in the process is hexavalent chromium. The proper exhaust ventilation equipment and fume-extraction torches are recommended, as well as suitable protective clothing and respiratory protection for operators.