Ramor® 500

Descargar ficha de datos

Seleccionar idioma

Get datasheet by email
Close

Get datasheet by email

    Descripción general del producto

    The ballistic protection steel with high hardness.

    Ramor® 500 is a ballistic protection steel of high hardness, available in thicknesses of 2.0 ‑ 30.0 mm (0.079‑1.18″) and hardnesses of 490‑560 HBW.

    Ramor® 500 is available as cut-to-length sheet in thicknesses of 2.0 ‑ 6.5 mm (0.079‑0.256″) and as plate in thicknesses of 6.0 ‑ 30.0 mm (0.236‑1.18″). Delivered in quenched condition, Ramor® 500 is not intended for further heat treatment.

    Propiedades mecánicas

    Ocultar/mostrar columnas específicas Editar
    Seleccionar columnas para mostrar
      Espesor
      (mm)
      Dureza
      (HBW)
      Ramor® 500 2.0 - 30.0 490 - 560
      Comparar parámetros

      Seleccione un parámetro para comparar

      Comparativa

        Mechanical Testing

        Brinell hardness test according to EN ISO 6506-1 on each heat treatment individual/coil.

        Hardness is measured on a milled surface 0.3-2 mm below plate surface.

        Composición química (análisis de colada)

        Ocultar/mostrar columnas específicas Editar
        Seleccionar columnas para mostrar
          C
          (max %)
          Si
          (max %)
          Mn
          (max %)
          P
          (max %)
          S
          (max %)
          Cr
          (max %)
          Ni
          (max %)
          Mo
          (max %)
          B
          (max %)
          0.35 0.70 1.5 0.015 0.010 1.00 2.0 0.70 0.005
          Comparar parámetros

          Seleccione un parámetro para comparar

          Comparativa

            El acero es de grano fino. El fósforo y el azufre no son elementos de aleación intencionados.

            Tolerancias

            More details are given on www.ssab.com.

            Espesor

            Ocultar/mostrar columnas específicas Editar
            Seleccionar columnas para mostrar
              Product Type Espesor
              (mm)
              Tolerancias
              (mm)
              Chapa 2.00 - 4.00 - 0.0 / + 0.36
              Chapa 4.01 - 5.00 - 0.0 / + 0.40
              Chapa 5.01 - 6.00 - 0.0 / + 0.42
              Chapa 6.01 - 6.50 - 0.0 / + 0.44
              Chapa gruesa 6.0 - 7.9 - 0.0 / + 0.8
              Chapa gruesa 8.0 - 14.9 - 0.0 / + 1.0
              Chapa gruesa 15.0 - 24.9 - 0.0 / + 1.2
              Chapa gruesa 25.0 - 30.0 - 0.0 / + 1.4
              Comparar parámetros

              Seleccione un parámetro para comparar

              Comparativa

                Largo y ancho

                Sheets are delivered with mill edges cut as standard.

                • Tolerances conform to EN 10 051 or to SSAB´s standard after agreement.

                Plate delivered according to SSAB’s dimension program.

                • Tolerances conform to EN 10 029 or to SSAB’s standard after agreement.
                • Dimensional tolerances for plate with mill edge according to special agreement. 

                Formato

                Tolerancias de conformidad con la norma EN 10029 para chapa gruesa y con la norma EN 10051 para chapa.

                Planitud

                Tolerances according to SSAB’s flatness tolerances which are more restrictive than EN 10 029 Class N (steel type L) and EN 10 051.

                Ocultar/mostrar columnas específicas Editar
                Seleccionar columnas para mostrar
                  Product Type Regla 1000
                  (mm)
                  Chapa 6
                  Chapa gruesa 6
                  Comparar parámetros

                  Seleccione un parámetro para comparar

                  Comparativa

                    Product Type
                    Chapa
                    Regla 1000
                    (mm)
                    6
                    Product Type
                    Chapa gruesa
                    Regla 1000
                    (mm)
                    6

                    Propiedades superficiales

                    De conformidad con la norma EN 10163-2, clase B, subclase 3.

                    Condiciones de entrega

                    Ramor is delivered in quenched condition.