Strenx 1300 E/F

Strenx® 1300

The ultra-high-strength steel at 1300 MPa

Strenx® 1300 is an ultra-high-strength structural steel with a minimum yield strength of 1300 MPa.

Typical applications include load-carrying structures that place very high demands on low weight. SSAB developed Strenx® 1300 for building the lightest possible steel solutions or providing an alternative to other materials. 

Strenx® 1300 benefits include:

  • Good weldability with excellent HAZ strength and toughness
  • Exceptional consistency within a plate guaranteed by close tolerances
  • High impact toughness which provides for good resistance to fractures
  • Superior bendability and surface quality

Ce este oțelul structural, de înaltă rezistență

SSAB expertise helps crane manufacturer develop cranes that can take the strain

Customer case
SSAB expertise helps crane manufacturer develop cranes that can take the strain

Dimension Range

Strenx® 1300 E/F is available as plate in thicknesses of 4.0 – 15.0 mm. Strenx® 1300 E/F is available in widths up to 2900 mm and lengths up to 14630 mm depending on thickness. More detailed information on dimensions is provided in the dimension program.

Available Standards

EN 10029

EN 10163-2

Strenx® 1300 E/F

Strenx® 1300 E/F

UTILIZARE
DIMENSIUNI
STANDARDE
FIȘĂ TEHNICĂ
UTILIZARE

Structural

Low temperatures (down to -60°)

DIMENSIUNI

T: 4 - 15 mm

W: Up to 2900 mm

L: Up to 14630 mm

STANDARDE

EN 10029

EN 10163-2

FIȘĂ TEHNICĂ