Hardenable boron steel for the automotive industry. Docol PHS 2000 steels are optimized for parts and components that are manufactured by direct or indirect hot stamping. Applications include safety parts such as bumper systems, door impact beams, and B-pillar reinforcements.
Cold rolled / UC: thickness 1.00-2.10 mm, width up to 1515 mm.
Hot rolled / UC*: thickness 2.00-4.00 mm, width up to 1600 mm.
Slit strip and cut to length sheets are available upon request.
*Available upon request.
Standard | Condition | Test direction |
Typical yield strength Rp0.2 (MPa) |
Typical tensile strength Rm (MPa) | Typical elongation A80 (%) |
Typical elongation A5 (%) |
|
---|---|---|---|---|---|---|---|
Docol PHS FH 2000 | SSAB | Full Hard | T | 980 | 1100 | 4 | — |
Docol PHS CR 2000 | SSAB | As delivered Annealed | T | 330 | 530 | 26 | — |
SSAB | Hot stamped 1) | T | 1380 | 2040 | 5 | — | |
Docol PHS HR 2000 | SSAB | Hot rolled | T | 490 2) | 690 | 18 | 22 |
SSAB | Hot stamped 1) | T | 1360 2) | 2040 | 6 | 7 | |
Docol PHS HR 2000+A | SSAB | Annealed | T | 330 2) | 540 | 27 | 31 |
1) Properties depend on the process.
2) ReH is used instead of Rp0.2.
C (%) |
Si (%) |
Mn (%) |
P (max %) |
S (max %) |
Cr (max %) |
B (%) |
Nb+Ti (max %) |
---|---|---|---|---|---|---|---|
0.30 - 0.38 | 0.15 - 0.35 | 1.10 - 1.50 | 0.025 | 0.005 | 0.35 | 0.0010 - 0.0050 | 0.2 |
Cold rolled (UC): Tolerances in accordance to EN 10131.
Hot rolled (UC): Tolerances in accordance to EN 10051.
Customized dimensional and shape tolerances are available upon request.
Uncoated (UC): available as oiled.
All surface treatments are in accordance with RoHS directive (2011/65/EU) and do not contain Chromium VI (Cr6+). Surface treatments provide only temporary surface protection during transportation and storage. In order to avoid corrosion damages, care must be taken to keep the products dry during transportation and storage. If they become wet, they must be separated and situated so that they are dried quickly.
For information concerning fabrication, see SSAB´s brochures on www.ssab.com or consult Tech Support.
Appropriate health and safety precautions must be taken when bending, welding, cutting, grinding or otherwise working on the products.
¿Desea descubrir aplicaciones únicas de automoción, probar nuevos métodos de producción o crear componentes más ligeros que ahorren combustible y mejoren la resistencia a los impactos y la sostenibilidad?
Los clientes existentes de Docol® disfrutan de un acceso 24/7 a los datos de conformado que necesita para ayudarle en su selección y simulación de aceros avanzados de alta resistencia para automoción.