General Product Description

Hardenable boron steel for the automotive industry. Docol PHS 2000 steels are optimized for parts and components that are manufactured by direct or indirect hot stamping. Applications include safety parts such as bumper systems, door impact beams, and B-pillar reinforcements.

Dimension Range

Cold rolled / UC: thickness 1.00-2.10 mm, width up to 1515 mm.

Hot rolled / UC*: thickness 2.00-4.00 mm, width up to 1600 mm.

Slit strip and cut to length sheets are available upon request.

*Available upon request.

Mechanical Properties

Hide/Show specific columns Edit
Select columns to display
    Standard Condition Test direction
    Typical yield strength Rp0.2
    (MPa)
    Typical tensile strength Rm (MPa) Typical elongation A80
    (%)
    Typical elongation A5
    (%)
    Docol PHS FH 2000 SSAB Full Hard T 980 1100 4
    Docol PHS CR 2000 SSAB As delivered Annealed T 330 530 26
    SSAB Hot stamped 1) T 1380 2040 5
    Docol PHS HR 2000 SSAB Hot rolled T 490 2) 690 18 22
    SSAB Hot stamped 1) T 1360 2) 2040 6 7
    Docol PHS HR 2000+A SSAB Annealed T 330 2) 540 27 31
    Compare parameters

    Select one parameter to compare

    Comparison

      1) Properties depend on the process.

      2) ReH is used instead of Rp0.2.

      Chemical Composition (ladle analysis)

      Hide/Show specific columns Edit
      Select columns to display
        C
        (%)
        Si
        (%)
        Mn
        (%)
        P
        (max %)
        S
        (max %)
        Cr
        (max %)
        B
        (%)
        Nb+Ti
        (max %)
        0.30 - 0.38 0.15 - 0.35 1.10 - 1.50 0.025 0.005 0.35 0.0010 - 0.0050 0.2
        Compare parameters

        Select one parameter to compare

        Comparison

          Tolerances

          Cold rolled (UC): Tolerances in accordance to EN 10131.

          Hot rolled (UC): Tolerances in accordance to EN 10051.

          Customized dimensional and shape tolerances are available upon request.

          Surface Treatments

          Uncoated (UC): available as oiled.

          All surface treatments are in accordance with RoHS directive (2011/65/EU) and do not contain Chromium VI (Cr6+). Surface treatments provide only temporary surface protection during transportation and storage. In order to avoid corrosion damages, care must be taken to keep the products dry during transportation and storage. If they become wet, they must be separated and situated so that they are dried quickly.

          Fabrication and Other Recommendations

          For information concerning fabrication, see SSAB´s brochures on www.ssab.com or consult Tech Support.

          Appropriate health and safety precautions must be taken when bending, welding, cutting, grinding or otherwise working on the products.

          Docol® PHS steel product offer

          Docol® PHS 1500 press hardening

          Docol® PHS 1800 press hardening

          Docol® PHS 2000 press hardening

          Contenido relacionado