Docol® PHS 1500 press hardening

Download data sheet

General Product Description

Hardenable boron steel for the automotive industry. Available as both hot rolled and cold rolled. Docol PHS 1500 steels are specially developed for parts and components that are manufactured by direct or indirect hot stamping. Applications include safety parts such as door impact beams, bumper systems and B- pillar reinforcements.

Dimension Range

Cold rolled / UC: thickness 0.70-3.00 mm, width up to 1500 mm.

Hot rolled / UC: thickness 2.00-12.00 mm, width up to 1600 mm.

Slit strip and cut to length sheets are available upon request.

Mechanical Properties

Docol PHS FH 1500

Standard
SSAB
Condition
Full Hard
Test direction
T
Typical yield strength Rp0.2 (MPa)
960
Typical tensile strength Rm (MPa)
1060
Typical elongation A80
(%)
4
Typical elongation A5
(%)
—

Docol PHS CR 1500

Docol PHS HR 1500+A

Standard
SSAB
Condition
Annealed
Test direction
T
Typical yield strength Rp0.2 (MPa)
350 2)
Typical tensile strength Rm (MPa)
530
Typical elongation A80
(%)
25
Typical elongation A5
(%)
33

1) Properties depend on the process.

2) ReH is used instead of Rp0.2.

Chemical Composition (ladle analysis)

C
(%)
C
(%)
0.20 - 0.25
Si
(%)
0.15 - 0.35
Mn
(%)
1.00 - 1.35
P
(max %)
0.025
S
(max %)
0.005
Cr
(max %)
0.35
B
(%)
0.0020 - 0.0050

Tolerances

Cold rolled (UC): Tolerances in accordance to EN 10131.

Hot rolled (UC): Tolerances in accordance to EN 10051.

Customized dimensional and shape tolerances are available upon request.

Surface Treatments

Uncoated (UC): available as oiled.

All surface treatments are in accordance with RoHS directive (2011/65/EU) and do not contain Chromium VI (Cr6+). Surface treatments provide only temporary surface protection during transportation and storage. In order to avoid corrosion damages, care must be taken to keep the products dry during transportation and storage. If they become wet, they must be separated and situated so that they are dried quickly.

Fabrication and Other Recommendations

For information concerning fabrication, see SSAB´s brochures on www.ssab.com or consult Tech Support.

Appropriate health and safety precautions must be taken when bending, welding, cutting, grinding or otherwise working on the products.

Docol® PHS steel product offer

Docol® PHS 1500 press hardening

Ver producto

Docol® PHS 1800 press hardening

Ver producto

Docol® PHS 2000 press hardening

Ver producto

Contenido relacionado

Existencias de materiales de prueba

¿Desea descubrir aplicaciones únicas de automoción, probar nuevos métodos de producción o crear componentes más ligeros que ahorren combustible y mejoren la resistencia a los impactos y la sostenibilidad?

Más información

Datos de conformado para aceros AHSS Docol®

Los clientes existentes de Docol® disfrutan de un acceso 24/7 a los datos de conformado que necesita para ayudarle en su selección y simulación de aceros avanzados de alta resistencia para automoción.

Más información