Docol® 1000CP is made for cold forming and allows for a tight bending radius on high-strength applications. These steels are characterized by both a high yield strength and an improved cleanliness, which allows for a tight radius.

Dimension Range

Cold rolled / UC, EG thickness 0.50-2.10 mm, width up to 1527 mm.

Cold rolled / GI: thickness 0.95-2.00 mm, width up to 1250 mm.

Slit strip and cut to length sheets are available upon request.

Grade and coating specific restrictions on available dimensions may occur.