The pre-hardened, exceptionally clean engineering and tool steel.
Toolox® 40 is a pre-hardened steel suitable for engineering components and mold applications. It possesses good dimensional stability after machining.
Toolox® 40 features the same machinability as the conventional P20/W.Nr 1.2311 steel, despite its nearly 100 HBW higher nominal hardness, in combination with the renowned high dimensional stability of Toolox®. This makes Toolox® 40 your ideal choice in engineering components that require higher strength, or in molds and dies that demand higher wear resistance.
1) Se mide la dureza, conforme a EN ISO 6506-1, en una superficie fresada de entre 0,5 y 2 mm por debajo de la superficie de la chapa.
1) Ensayo de impacto según EN 10 025, EN ISO 148 con un percutor de 2 mm.
Ultrasonic inspection is carried out according to : EN 10 160 with extra demands according to specification SSAB V6.
More details are given in SSAB’s brochure Toolox® Guarantees and on www.toolox.com.
Tolerances according to Toolox® Thickness Guarantee.
Toolox® Guarantees meets the requirements of EN 10029 Class C but offers more narrow tolerances.
Tolerances according to EN 10029.
Tolerances are according to Toolox® Flatness Guarantees, which are more restrictive than EN 10029 Class N (steel type L).
De conformidad con la norma EN 10163-2, clase B, subclase 3.
Quenched and Tempered at a minimum temperature of 590 °C.
On delivery from SSAB the plates meet the following specifications:
Delivery requirements can be found in SSAB’s brochure Toolox® Guarantees or at www.toolox.com.