Strenx 900 Plus

Strenx® 900 Plus

Strenx® 900 Plus is a structural steel that guarantees a minimum yield strength of 900 MPa.

Strenx® 900 Plus provides a unique combination of strength and toughness together with first-rate workshop properties.

Typical applications include load-bearing structures, where low weight is needed. Strenx® 900 Plus meets the requirements of EN 10 025-6 for the S890QL grade.

Benefits include:

• High impact toughness which provides for good resistance to fractures
• Superior bendability and surface quality
• Weldability with excellent HAZ strength and toughness
• Exceptional consistency within a sheet guaranteed by close tolerances

Dimension Range

Strenx® 900 Plus is available as cut to length sheets in thicknesses of 2.0 - 8.0 mm. Strenx 900 Plus is available in widths up to 1600 mm and lengths up to 16000 meters depending on thickness. Please contact your sales representative for more information regarding dimensions.

 

Available Standards

EN 10025-6

EN 10051

EN 10163-2

Strenx® 900 Plus

Strenx® 900 Plus

UTILIZARE
DIMENSIUNI
STANDARDE
FIȘĂ TEHNICĂ
UTILIZARE

Structural

DIMENSIUNI

T: 2 - 8 mm

W: Up to 1600 mm

L: Up to 16000 mm

STANDARDE

EN 10025-6

EN 10051

EN 10163-2

FIȘĂ TEHNICĂ