Strenx 700 OME

Strenx® 700 OME

A structural steel developed for use in demanding load-bearing structures within the Offshore and Marine Industry.

Strenx® 700 OME exceeds the requirements of S690QL, EN 10 025-6. Strenx® 700 OME can be ordered with dual steel grades certificate, where the additional steel grade is defined and approved by one of the Classification Societies listed below.

The dual certification offers You the benefits of excellent mechanical properties, extra tight tolerances, formability and consistency of SSAB Strenx® Guarantees.

 

Classification society:

 

- American Bureau of Shipping                      AB EQ70, 4.8 to 130 mm thickness.

- DNV - GL                                                          NV E690, VL E690, 6 to 80 mm thickness.

- Lloyds Register                                               LR EH 69, 8 to 80 mm thickness.

Dimension Range

Strenx® 700 OME is available as plate in thicknesses of 4.0 – 130.0 mm and available in widths up to 3350 mm and lengths up to 14630 mm depending on thickness. More detailed information on dimensions is provided in the dimension program for Strenx® 700 E/F at www.ssab.com.

Available Standards

EN 10025-6

EN 10029

EN 10163-2

Strenx® 700 OME

Strenx® 700 OME

UTILIZARE
DIMENSIUNI
STANDARDE
FIȘĂ TEHNICĂ
UTILIZARE

Structural

Low temperatures (down to -60°)

DIMENSIUNI

T: 4 - 130 mm

W: Up to 3350 mm

L: Up to 14630 mm

STANDARDE

EN 10025-6

EN 10029

EN 10163-2

FIȘĂ TEHNICĂ