Strenx 650MC D/E

Strenx® 650MC

The high-strength structural steel at 650 MPa

Strenx® 650MC is a hot-rolled structural steel made for cold forming, with a minimum yield strength of 650 MPa for stronger and lighter structures.

Strenx® 650MC meets or exceeds the requirements of S650MC in EN 10149-2.

Typical applications include a wide range of components and parts, such as demanding load-bearing structures. Strenx® 650MC comes in coils, slit coils or cut-to-length sheets.

Ce este oțelul structural, de înaltă rezistență

Customer case

Dimension Range

Strenx® 650MC D/E is available in thicknesses of 2.00-10.00 mm and widths up to 1600 mm as coils, slit coils or cut to length sheets in lengths up to 16 meters.

 

Available Standards

EN 10149-2

EN 10051

EN 10163-2

Strenx® 650MC D/E

Strenx® 650MC D/E

UTILIZARE
DIMENSIUNI
STANDARDE
FIȘĂ TEHNICĂ
UTILIZARE

Structural

DIMENSIUNI

T: 2 - 10 mm

W: Up to 1600 mm

L: Up to 16000 mm

STANDARDE

EN 10149-2

EN 10051

EN 10163-2

FIȘĂ TEHNICĂ