P200

P200

A thick-layer, color coated steel product

SSAB’s P200 is suitable for profiled sheet for roofing, wall claddings, associated fittings and facades.

SSAB´s Plastisol 200 is a thick, color coated product with an embossed surface. It combines high wear resistance with high durability against corrosion. P200 is easy to process and can be bent without restrictions.

The product has superior durability when exposed to people walking on the roof and other roof stresses, and features excellent corrosion protection.

The reverse side of the sheet is painted as standard with a two-layer grey backside coating.

SSAB color coated products comply with current REACH regulations and are fully free of chromates. GreenCoat® color coated steels are all manufactured according to EN 10169 + A1.

Detalii produse

În această secțiune veți găsi o gamă largă de produse vopsite GreenCoat® pentru acoperișuri, inclusiv detalii tehnice.

P200

P200

PROPRIETĂȚI PRINCIPALE
ACOPERIRE
PALETĂ CROMATICĂ
FIȘĂ TEHNICĂ
PROPRIETĂȚI PRINCIPALE

Mechanical durability

Corrosion resistance

Wide color offering

ACOPERIRE

Embossed

PALETĂ CROMATICĂ

  • White
    RR120 / SS----

  • Anthracite Grey
    RR2H8 / SS0087

  • Nordic Night Black
    RR33 / SS0015

  • Walnut Brown
    RR32 / SS0387

FIȘĂ TEHNICĂ