GreenCoat PLX Pro BT

GreenCoat PLX Pro BT

The product developed specifically for tinsmiths

GreenCoat PLX Pro BT is a highly formable product workable at temperatures down to -15°C.

GreenCoat PLX Pro BT is a product for long strip roofing. This product has been developed together with tinsmiths in order to obtain optimum product properties combined with Nordic quality steel and an excellent coating. The result is a unique, premium product for tinsmiths.

The highly formable steel PLX in combination with our first-class BT coating makes it a premium product for premium applications. The PLX steel has practically no spring back, which provides for very tight folding. GreenCoat PLX Pro BT can be formed by hand and is workable at temperatures down to – 15°C, allowing for year round installation at lower costs.

Additionally, the product is manufactured according to the BT patent (Bio-based Technology) and therefore holds a high environmental position. In BT coatings, where a substantial portion of the traditional fossil oil is replaced by Swedish rapeseed oil, which is unique on the market. GreenCoat PLX Pro BT is coated with 350 g zinc/m² and is provided with a BT color coating.

SSAB holds a worldwide patent for this coating technology. GreenCoat PLX Pro BT is a high quality product ensuring excellent corrosion and UV resistance properties.

The reverse side of the sheet is painted with a two-layer limestone turquoise backside coating. SSAB color coated products comply with current REACH regulations and are fully free of chromates. GreenCoat® color coated steels are all manufactured according to EN 10169 + A1.

GreenCoat PLX – alegerea acoperitorilor de case

Carl Cross, de la Zinc and Copper Roofing Ltd (Regatul Unit), a instalat GreenCoat PLX pe un acoperiş şi ne împărtăşeşte gândurile sale. Urmăriţi filmul.

Detalii produse

În această secțiune veți găsi o gamă largă de produse vopsite GreenCoat® pentru acoperișuri, inclusiv detalii tehnice.

GreenCoat PLX Pro BT

GreenCoat PLX Pro BT

UTILIZARE
PROPRIETĂȚI PRINCIPALE
ACOPERIRE
PALETĂ CROMATICĂ
FIȘĂ TEHNICĂ
UTILIZARE

Roofing

PROPRIETĂȚI PRINCIPALE

Enhanced formability

Outdoor durability

Mechanical durability

Bio-based Technology (BT)

Corrosion resistance

Wide color offering

ACOPERIRE

Regular

Matt

PALETĂ CROMATICĂ

  • Nordic White
    RR1H3 / SS0020

  • Winter White
    RR20 / SS0005

  • Snow White
    RR19 / SS0001

  • Arctic White
    RR1L6 / SS0002

  • Polar White
    RR--- / SS6080

  • Powder White
    RR--- / SS0021

  • Limestone Grey
    RR268 / SS0022

  • Goosewing Grey
    RR2H5 / SS0461

  • Gravel Grey
    RR--- / SS0241

  • Quarry Grey
    RR287 / SS0244

  • Rock Grey
    RR237 / SS0061

  • Anthracite Grey
    RR2H8 / SS0087

  • Mountain Grey
    RR23 / SS0036

  • Summit Grey
    RR--- / SS0454

  • Cliff Grey
    RR288 / SS0455

  • Nordic Night Black
    RR33 / SS0015

  • Walnut Brown
    RR32 / SS0387

  • Acorn Brown
    RR827 / SS0434

  • Coffee Brown
    RR820 / SS0384

  • Cottage Red
    RR29 / SS0758

  • Brick Red
    RR7F2 / SS0742

  • Fire Brick Red
    RR7G9 / SS0757

  • Harvest Yellow
    RR24 / SS0189

  • Silver Fir Green
    RR5J3 / SS0975

  • Leaf Green
    RR594 / SS0874

  • Pine Green
    RR11 / SS0830

  • Olive Leaf Green
    RR5H8 / SS6033

  • Lake Blue
    RR35 / SS0558

  • Metallic Silver
    RR40 / SS0045

  • Metallic Sterling
    RR974 / SS6045

  • Metallic Dark Silver
    RR41 / SS0044

  • Dark Silver Metallic
    RR977 / SS6015

  • Metallic Copper
    RR979 / SS0778

FIȘĂ TEHNICĂ