GreenCoat Crown BT, available in matt and regular finishes, offers high color retention, color fastness and durability for tile profiles, modular roofs and lock form roofs. It can also be used in sandwich panels and wall cladding as it keeps its good looks over time and will stand up well to corrosion.

The product uses a bio-based coating which uses a substantial portion of Swedish rapeseed oil instead of fossil oil, which is unique on the market. SSAB holds a worldwide patent for this coating technology.

GreenCoat Crown BT with a matt finish delivers the highest level of color and gloss repeatability as well as formability. It is therefore particularly recommended for modular roofing. A structured surface helps protect further against mechanical wear and is easy to handle during manufacturing.

SSAB color coated products comply with current REACH regulations and are fully free of chromates. GreenCoat® color coated steels are all manufactured according to EN 10169 + A1.

 

Detalii produse

În această secțiune veți găsi o gamă largă de produse vopsite GreenCoat® pentru acoperișuri, inclusiv detalii tehnice.

GreenCoat Crown BT

GreenCoat Crown BT

UTILIZARE
PROPRIETĂȚI PRINCIPALE
ACOPERIRE
PALETĂ CROMATICĂ
FIȘĂ TEHNICĂ
UTILIZARE

Roofing

Facades

PROPRIETĂȚI PRINCIPALE

Outdoor durability

Bio-based Technology (BT)

Enhanced formability

Enhanced color and gloss repeatability

ACOPERIRE

Regular

Matt

PALETĂ CROMATICĂ

  • Nordic White
    RR1H3 / SS0020

  • Snow White
    RR19 / SS0001

  • Pebble Grey
    RR21 / SS0011

  • Anthracite Grey
    RR2H8 / SS0087

  • Mountain Grey
    RR23 / SS0036

  • Slate Grey
    RR2H3 / SS0534

  • Nordic Night Black
    RR33 / SS0015

  • Walnut Brown
    RR32 / SS0387

  • Chestnut Brown
    RR887 / SS0435

  • Acorn Brown
    RR827 / SS0434

  • Cottage Red
    RR29 / SS0758

  • Tile Red
    RR750 / SS0760

  • Brick Red
    RR7F2 / SS0742

  • Pine Green
    RR11 / SS0830

FIȘĂ TEHNICĂ