GreenCoat Pural Farm BT

GreenCoat Pural Farm BT

High end product with Bio-based Technology (BT) specially developed for agricultural buildings

GreenCoat Pural Farm BT offers the highest level of durability and good wear resistance.

GreenCoat Pural Farm BT offers highest level of durability for agricultural buildings. GreenCoat Pural Farm BT with two-layer epoxy reverse side coating is used for sandwich panels in insulated and heated buildings e.g. chicken houses. Double sided GreenCoat Pural Farm BT is used for profiles in non-insulated and cold buildings e.g. cowsheds and open storages.

Pural coatings have been used and tested over 20 years in harsh conditions. The chemical composition of the coating is optimized to resist weathering, resulting in excellent UV resistance and corrosion properties. In addition GreenCoat Pural Farm BT gives excellent chemical resistance. The slightly structured surface helps protect against mechanical wear and is easy to handle during manufacturing. In addition GreenCoat

Pural Farm BT possesses excellent forming properties.

The product uses a bio-based coating which uses a substantial portion of Swedish rapeseed oil instead of fossil oil, which is unique on the market. SSAB holds a worldwide patent for this coating technology.

SSAB color coated products comply with current REACH regulations and are fully free of chromates. GreenCoat® color coated steels are all manufactured according to EN 10169 + A1.

Detalii produse

În această secțiune veți găsi o gamă largă de produse vopsite GreenCoat® pentru acoperișuri, inclusiv detalii tehnice.

GreenCoat Pural Farm BT

GreenCoat Pural Farm BT

UTILIZARE
PROPRIETĂȚI PRINCIPALE
ACOPERIRE
PALETĂ CROMATICĂ
FIȘĂ TEHNICĂ
UTILIZARE

Facades

PROPRIETĂȚI PRINCIPALE

Outdoor durability

Bio-based Technology (BT)

Mechanical durability

Enhanced formability

Corrosion resistance

ACOPERIRE

Regular

PALETĂ CROMATICĂ

  • Stone Grey
    RR22 / SS0554

  • Rock Grey
    RR237 / SS0061

  • Mountain Grey
    RR23 / SS0036

  • Slate Grey
    RR2H3 / SS0534

  • Nordic Night Black
    RR33 / SS0015

  • Walnut Brown
    RR32 / SS0387

  • Chestnut Brown
    RR887 / SS0435

  • Hazelnut Brown
    RR8H2 / SS0426

  • Cottage Red
    RR29 / SS0758

  • Brick Red
    RR7F2 / SS0742

  • Harvest Yellow
    RR24 / SS0189

  • Pine Green
    RR11 / SS0830

  • Lake Blue
    RR35 / SS0558

FIȘĂ TEHNICĂ