Docol® 650LA high strength low alloy

More about high strength low alloy steel

Download data sheet

Select Language

Get datasheet by email
Close

Get datasheet by email

En esta página

General Product Description

The Docol 650LA is a high-strength low-alloy steel that offer consistent properties for modern, rapid production methods. Typical applications include components and parts such as load-bearing structures, for example chassis. Docol HR650LA-UC can after agreement be adapted and delivered as dual certified with S650MC according to EN 10149-2.

Dimension Range

Hot rolled / UC: thickness 2.00-6.00 mm, width up to 1600 mm.

Slit strip and cut to length sheets are available upon request.

Grade and coating specific restrictions on available dimensions may occur.

Mechanical Properties

Hide/Show specific columns Edit
Select columns to display
    Standard Coating Test direction
    Yield strength Rp0.2
    (MPa)
    Tensile strength Rm
    (MPa)
    Elongation A80 1)
    (min %)
    Elongation A5 2)
    (min %)
    Min. inner bending radius for a 90° bend
    Docol HR​650LA SSAB UC L 650 - 780 700 - 850 12 14 1.2 x t
    Compare parameters

    Select one parameter to compare

    Comparison

      1) A80 value applies for thicknesses < 3.00 mm.

      2) A5 value applies for thicknesses ≥ 3.00 mm.

      Chemical Composition (ladle analysis)

      Hide/Show specific columns Edit
      Select columns to display
        Coating C
        (max %)
        Si
        (max %)
        Mn
        (max %)
        P
        (max %)
        S
        (max %)
        Al
        (%)
        Ti
        (max %)
        Nb
        (max %)
        Cu
        (max %)
        Docol HR​650LA UC 0.12 0.60 2.00 0.025 0.010 From 0.015 0.15 0.09 0.20
        Compare parameters

        Select one parameter to compare

        Comparison

          Tolerances

          Hot rolled (UC): Tolerances in accordance to EN 10051.

          Customized dimensional and shape tolerances are available upon request.

          Surface Treatments

          Uncoated (UC): available as oiled.

          All surface treatments are in accordance with RoHS directive (2011/65/EU) and do not contain Chromium VI (Cr6+). Surface treatments provide only temporary surface protection during transportation and storage. In order to avoid corrosion damages, care must be taken to keep the products dry during transportation and storage. If they become wet, they must be separated and situated so that they are dried quickly.

          Fabrication and Other Recommendations

          For information concerning fabrication, see SSAB´s brochures on www.ssab.com or consult Tech Support.

          Appropriate health and safety precautions must be taken when bending, welding, cutting, grinding or otherwise working on the products.

          Docol® High Strength Low Alloy steel product offer

          Docol® 420LA high strength low alloy

          Docol HR100XF

          Docol HR110XF

          Docol® S600MC high strength low alloy

          Docol® S650MC high strength low alloy

          Docol® S700MC high strength low alloy

          Docol® S900MC high strength low alloy

          Docol S960MC

          Docol® 460LA high strength low alloy

          Docol® 500LA high strength low alloy

          Docol® 550LA high strength low alloy

          Docol® 600LA high strength low alloy

          Docol® 650LA high strength low alloy

          Docol® 700LA high strength low alloy

          Contenido relacionado