Structural
T: -400 - 2500 Inches
EN 10029
Structural
T: 2 - 10 mm
W: Up to 1600 mm
L: Up to 16000 mm
EN 10051
EN 10163-2 Class A, Subclass 3
Structural
T: 2 - 10 mm
W: Up to 1600 mm
L: Up to 16000 mm
EN 10051
EN 10163-2 Class A, Subclass 3
Structural
T: 2 - 10 mm
W: Up to 1600 mm
L: Up to 16000 mm
EN 10149-2
EN 10051
EN 10163-2
Structural
T: 2 - 10 mm
W: Up to 1600 mm
L: Up to 16000 mm
EN 10149-2
EN 10051
EN 10163-2
Structural
Low temperatures (down to -60°)
T: 4 - 160 mm
W: Up to 3350 mm
L: Up to 14630 mm
EN 10025-6
EN 10029
EN 10163-2
Structural
T: 2 - 10 mm
W: Up to 1600 mm
L: Up to 16000 mm
EN 10051
EN 10163-2
EN 10149-2
Structural
Low temperatures (down to -60°)
T: 3 - 12 mm
W: Up to 1525 mm
L: Up to 12300 mm
EN 10051
EN 10163-2
EN 10149-2
Structural
T: 0.7 - 2.1 mm
W: Up to 1500 mm
L: Up to 8500 mm
EN 10131
Structural
Low temperatures (down to -60°)
T: 4 - 130 mm
W: Up to 3350 mm
L: Up to 14630 mm
EN 10025-6
EN 10029
EN 10163-2
Structural
Low temperatures (down to -60°)
T: 4 - 120 mm
W: Up to 3350 mm
L: Up to 14630 mm
EN 10025-6
EN 10029
EN 10163-2
Structural
T: 3 - 10 mm
W: Up to 1600 mm
L: Up to 13000 mm
EN 10051
EN 10149-2
EN 10163-2
Structural
T: 2 - 8 mm
W: Up to 1600 mm
L: Up to 16000 mm
EN 10025-6
EN 10051
EN 10163-2
Structural
T: 4 - 120 mm
W: Up to 3350 mm
L: Up to 14630 mm
EN 10025-6
EN 10029
EN 10163-2
Structural
T: 3 - 10 mm
W: Up to 1600 mm
L: Up to 13000 mm
EN 10051
EN 10163-2
EN 10149-2
Structural
T: 2 - 8 mm
W: Up to 1600 mm
L: Up to 16000 mm
EN 10025-6
EN 10051
EN 10163-2
Structural
T: 0.8 - 2.1 mm
W: Up to 1500 mm
L: Up to 8500 mm
EN 10131
Structural
Low temperatures (down to -60°)
T: 4 - 40 mm
W: Up to 3200 mm
L: Up to 14630 mm
EN 10029
EN 10163-2
Structural
T: 4 - 8 mm
W: Up to 1600 mm
L: Up to 16000 mm
EN 10051
EN 10163-2
Structural
T: 3 - 8 mm
W: Up to 1700 mm
L: Up to 16000 mm
EN 10051
EN 10163-2
Structural
T: 0.7 - 2.1 mm
W: Up to 1500 mm
L: Up to 8500 mm
EN 10131
Structural
Low temperatures (down to -60°)
T: 4 - 15 mm
W: Up to 2900 mm
L: Up to 14630 mm
EN 10029
EN 10163-2
T: 3 - 10 mm
D: 33.7 - 323.9 mm
W: Up to 300 mm
L: Up to 18000 mm
EN 1090-2
10219
T: 3 - 10 mm
D: 33.7 - 323.9 mm
W: Up to 300 mm
L: Up to 18000 mm
EN 1090-2
10219
T: 2 - 6.3 mm
D: 25 - 133 mm
L: Up to 12000 mm
EN 10210-2
T: 4 - 6 mm
D: 114.3 - 244.5 mm
W: Up to 160 mm
L: Up to 18000 mm
10219
T: 4 - 6 mm
D: 76.1 - 219.1 mm
W: Up to 160 mm
L: Up to 18000 mm
10219
T: 2 - 6.3 mm
D: 25 - 133 mm
L: Up to 12000 mm
EN 10210-2