Toolox 44
Toolox 44 engineering and tool steel

Toolox® 44

The pre-hardened steel for extrusion dies and engineering components

Toolox® 44 pre-hardened steel is suitable for extrusion dies and engineering components that require high strength. It possesses good workshop properties.

Toolox® 44 is a pre-hardened engineering and tool steel. Despite its high hardness, Toolox® 44 combines very good machinability with dimensional stability during machining.

Its nominal 450 HBW/45 HRC hardness makes Toolox® 44 your ideal choice for demanding mold and die applications. The high steel cleanliness gives Toolox® 44 very good polishing, A2 gloss, and texturing capabilities.

In applications that demand additional surface hardness to counteract wear, you can nitride and PVD coat Toolox® 44 to customize the mold or die properties. Surface engineering can be carried out as long as the deposition temperature does not exceed 590°C (1,094°F).


Contact us

High-strength engineering tool steel

The new generation of tool steel.

Toolox 44 extends die life

Toolox® 44 extends die life

Learn more

Toolox® 44 in the automotive industry

Learn more
Toolox customer cases

Dimension Range

Toolox® 44 is available as plates in thicknesses between 6.0 - 130.0 mm. Other dimensions can be available on request.

 

Available Standards

EN 10029

Toolox® 44

Toolox® 44

USED FOR
DIMENSIONS
STANDARDS
DATA SHEET
USED FOR

Tooling & Engineering

High temperatures (up to 590°C)

DIMENSIONS

STANDARDS

EN 10029

DATA SHEET