180 180
GreenCoat Pural BT
GreenCoat Pural

GreenCoat Pural BT

Proven durability that outlasts the harshest weather

Today, we are proud to inform that after years of research and testing, GreenCoat Pural is available as an upgraded version with a bio-based (BT) coating. The patented BT solution includes a substantial amount of Swedish rapeseed oil instead of fossil fuel oils in the coating – for greener living. The upgraded product name will be: GreenCoat Pural BT. GreenCoat Pural BT, available in regular and matt finishes in many colors, offers the highest level of durability for roofing applications.

Pural coatings have been used and tested over 20 years in harsh conditions. The chemical composition of the coating is optimized to resist weathering, resulting in excellent UV resistance and corrosion properties. The slight structure makes the surface very resistant against wear and tear. The new coating is also more flexible than the previous version of Pural. We are so confident with the performance that we will now by this change also increase the coating guarantee by 5 years.

The reverse side of the sheet is painted with a two-layer grey backside coating which further enhances the corrosion resistance.

GreenCoat Pural BT continues to offer the following characteristics:

  • The highest level of durability, thus a increased coating guarantee up to 25 years.
  • Wide range of colors inspired by Nordic nature.
  • Availability in regular gloss and matt finishes.
  • Excellent UV resistance: Ruv4 and wear resistance: RC5.
  • Excellent forming properties enabling very demanding folding, down to -15 °C.

SSAB color coated products comply with current REACH regulations and are fully free of chromates. GreenCoat® color coated steels are all manufactured according to EN 10169 + A1.

Product details

In this section, you will find the wide range of GreenCoat® color coated products for roofing applications including technical details.
Learn more

Product details

In this section, you will find our wide product offering with our Nordic quality steels and zinc coatings recommended for different applications. Details about product dimensions are also available.

Main applications  Recommended product*  Recommended steels Recommended Zinc mass Min thickness**  Width range*** 
Roofing, tinsmith
GreenCoat PLX Pro BT PLX Z350 0.60 mm 1000-1500 mm
 GreenCoat FAP Pro BT FAP  Z350  0.60 mm 1000-1500 mm 
GreenCoat PLX Legacy PLX Z350 0.60 mm 1000-1500 mm
           
Roofing, tiles & profiles GreenCoat Pural BT S280GD, S320GD, S350GD
Z275 0.50 mm 1000-1500 mm
GreenCoat Pro BT S280GD, S320GD, S350GD
Z275 0.50 mm 1000-1500 mm
GreenCoat Mica BT S280GD, S320GD, S350GD
Z275 0.50 mm 1000-1500 mm
GreenCoat Crown BT S280GD, S320GD, S350GD
Z275 0.50 mm 1000-1300 mm
Rough Matt Polyester S280GD, S320GD, S350GD
 Z275 0.45 mm  1000-1424 mm
Polyester S280GD-S350GD, DX51D
Z275 0.42 mm 1000-1500 mm
           
Roofing, modular GreenCoat Crown BT S280GD, S320GD, S350GD Z275 0.50 mm 1000-1300 mm
           
Rain water systems GreenCoat RWS Pro FAX, PLX Z275 0.50 mm 1000-1500 mm
           
Facades GreenCoat Hiarc S280GD, S320GD, DX51D 
Z275 0.50 mm 1000-1500 mm
GreenCoat Hiarc Max S280GD, S320GD, DX51D 
Z275 0.50 mm 1000-1500 mm
GreenCoat Crown BT S280GD, S320GD
Z275 0.50 mm 1000-1300 mm
Polyester S280GD, S320GD, DX51D 
Z275 0.42 mm 1000-1500 mm
           
Indoor applications Polyester Indoor S250GD-S350GD, DX51D 
Z100 0.40 mm 1000-1424 mm
GreenCoat Foodsafe BT S250GD-S350GD, DX51D 
Z100 0.50 mm 1000-1500 mm
Laminate Foodsafe S250GD-S350GD, DX51D 
Z275 0.42 mm 1000-1400 mm
Epoxy S250GD-S350GD, DX51D 
Z100 0.40 mm 1000-1500 mm

* In addition to these we have a wide range of so called custom made products. Please contact SSAB Europe Tech support.
** Please take into account the country specific building recommendations concerning the minimum thickness. If other thicknesses are required, please contact SSAB Tech Support. Max thickness is 1,5 mm.
*** Max width depends on steel thickness. If other steel dimensions are needed, please contact SSAB Tech Support.

GreenCoat coils

GreenCoat Pural BT

GreenCoat Pural BT

USED FOR
MAIN PROPERTIES
COATING
COLOR PALETTE
DATA SHEET
USED FOR

Roofing

MAIN PROPERTIES

Outdoor durability

Mechanical durability

Enhanced formability

Corrosion resistance

Wide color offering

Bio-based Technology (BT)

COATING

Regular

Matt

COLOR PALETTE

  • Winter White
    RR20 / SS0005

  • Snow White
    RR19 / SS0001

  • Concrete Grey
    RR292 / SS----

  • Pebble Grey
    RR21 / SS0011

  • Quarry Grey
    RR287 / SS0244

  • Stone Grey
    RR22 / SS0554

  • Rock Grey
    RR237 / SS0061

  • Anthracite Grey
    RR2H8 / SS0087

  • Mountain Grey
    RR23 / SS0036

  • Ridge Grey
    RR2F7 / SS0035

  • Slate Grey
    RR2H3 / SS0534

  • Nordic Night Black
    RR33 / SS0015

  • Walnut Brown
    RR32 / SS0387

  • Chestnut Brown
    RR887 / SS0435

  • Almond Brown
    RR30 / SS0187

  • Terra Brown
    RR31 / SS0433

  • Cottage Red
    RR29 / SS0758

  • Tile Red
    RR750 / SS0760

  • Brick Red
    RR7F2 / SS0742

  • Wine Red
    RR798 / SS5781

  • Harvest Yellow
    RR24 / SS0189

  • Silver Fir Green
    RR5J3 / SS0975

  • Leaf Green
    RR594 / SS0874

  • Pine Green
    RR11 / SS0830

  • Forest Green
    RR37 / SS0925

  • Lake Blue
    RR35 / SS0558

  • Metallic Silver
    RR40 / SS0045

  • Metallic Dark Silver
    RR41 / SS0044

  • Metallic Gold
    RR42 / SS----

  • Metallic Copper
    RR979 / SS0778

DATA SHEET