SSAB Form 07 is a mild steel intended for forming with the best conceivable properties in both drawing and stretch forming operations. SSAB Form 07 is used for a wide variety of applications including vehicle parts, refrigerators, electric radiators and water radiators.
SSAB Form 07 meets and exceeds the requirements of DC07 in EN 10130.
SSAB Form 07 is available in thicknesses of 0.50-3.00 mm and widths up to 1500 mm as coils, slit coils and as cut to length in lengths up to 8.5 meters.
Yield strength Rp0.2 (max MPa)  | Tensile strength Rm (MPa)  | Elongation A80 (min %)  | r90 (min)  | n90 (min)  | 
|---|---|---|---|---|
140 1)  | 250 - 310  | 44  | 2.3  | 0.23  | 
The mechanical properties are tested in the transversal direction.
1) For material delivered as cut to length sheets the maximum yield strength is 150 MPa.
C (max %)  | Si (max %)  | Mn (max %)  | P (max %)  | S (max %)  | Al (min %)  | Nb+Ti (max %)  | 
|---|---|---|---|---|---|---|
0.010  | 0.040  | 0.25  | 0.025  | 0.020  | 0.015  | 0.10  | 
SSAB Form cold rolled products are supplied with tolerances in accordance to EN 10131. More narrow thickness tolerances according to the SSAB standard are available upon request.
Cold rolled.
For information concerning fabrication, see SSAB´s brochures on www.ssab.com or consult Tech Support.
Appropriate health and safety precautions must be taken when bending, welding, cutting, grinding or otherwise working on the products.