    General Product Description

    SSAB Form 05 is a mild steel intended for forming with the best conceivable properties in both drawing and stretch forming operations. SSAB Form 05 is used for a wide variety of applications including vehicle parts, refrigerators, electric radiators and water radiators.

    Dimension Range

    SSAB Form 05 is available in thicknesses of 0.50-3.00 mm and widths up to 1500 mm as coils, slit coils and as cut to length in lengths up to 8.5 meters.

    Mechanical Properties

    Hide/Show specific columns Edit
    Select columns to display
      Yield strength Rp0.2
      (max MPa)
      Tensile strength Rm
      (MPa)
      Elongation A80 1)
      (min %)
      r90 2)
      (min)
      n90 2)
      (min)
      180 270 - 330 40 1.9 3) 0.20
      Compare parameters

      Select one parameter to compare

      Comparison

        The mechanical properties are tested in the transversal direction.

        1) When the thickness is less than or equal to 0.7 mm and greater than 0.5 mm, the minimum value for elongation is reduced by 2 units. For a thickness less than or equal to 0.5 mm, the minimum value is reduced by 4 units.

        2) The values of r90 and n90 only apply to products with a thickness equal to or greater than 0.5 mm

        3) When thickness is greater than 2mm the minimum value is reduced by 0.2.

        Chemical Composition (heat analysis)

        Hide/Show specific columns Edit
        Select columns to display
          C
          (max %)
          Si
          (max %)
          Mn
          (max %)
          P
          (max %)
          S
          (max %)
          Al
          (min %)
          Nb+Ti
          (max %)
          0.060 0.040 0.35 0.025 0.025 0.015 0.10
          Compare parameters

          Select one parameter to compare

          Comparison

            Tolerances

            SSAB Form cold rolled products are supplied with tolerances in accordance to EN 10131. More narrow thickness tolerances according to the SSAB standard are available upon request.

            Delivery Conditions

            Cold rolled.

            Fabrication and Other Recommendations

            For information concerning fabrication, see SSAB´s brochures on www.ssab.com or consult Tech Support.

            Appropriate health and safety precautions must be taken when bending, welding, cutting, grinding or otherwise working on the products.

            Contact Information

            www.ssab.com/contact