Ramor 600

Ramor® 600

The ballistic protection steel with extra-high hardness

​Ramor®/sup> 600 is a ballistic protection steel of extra-high hardness, nominal 600 HBW, available in thicknesses of 3‑6 mm (0.118‑0.236″).

Ramor® 600 is available as cut-to-length sheet in thicknesses of 3‑6 mm (0.118‑0.236″). Delivered in quenched condition, Ramor 600 is not intended for further heat treatment. Read more on SSAB armor and ballistic steels.

Dimension Range

Ramor 600 is available as cut-to-length sheet in thickness between 3.0 - 6.0 mm.

 

 

Available Standards

EN 10029

EN 10051

Ramor 600

Ramor 600

USED FOR
DIMENSIONS
STANDARDS
DATA SHEET
USED FOR

Armored

DIMENSIONS

T: 3 - 6 mm

STANDARDS

EN 10029

EN 10051

DATA SHEET