SSAB Laser® 250C
Advanced hot rolled structural steel for cold forming, optimized for laser cutting, with a minimum yield strength of 250 MPa.
SSAB Laser® 250C is the optimal steel for laser cutting and cold forming, with guaranteed flatness after laser cutting.
SSAB Laser® 250C is the result of total production process control. Every step of the way counts, from liquid iron to hot rolled plate and cut to length sheet. The chemical composition with low sulphur, phosphorous and silicon in combination with the perfected hot rolling process create the uniform and smooth microscale surface for optimal laser cutting.
SSAB Laser® 250C is dead-flat. Flatness, before and after laser cutting, is guaranteed to ≤ 3.0 mm/m.
SSAB Laser® 250C meets and exceeds the requirements of EN 10025-2 for S235J2C+N. Dual material certification and CE marking is available upon request. The SSAB Laser dimensional tolerances exceed the requirements of EN 10051 for hot rolled sheet and EN 10029 for thot rolled plate.
The SSAB Laser® product family consists of hot rolled plate and sheet and cold rolled sheet with yield strength levels up to 460 MPa. All products benefit from superior steel cleanliness, well balanced and consistent chemistry, optimized for laser cutting and narrow and consistent dimensional tolerances.