180
This website uses cookies to enhance your experience. By continuing to use this website you are agreeing to our
Cookie Policy
.
Brands & products
Steel selector
Download center
Support
Services
Contact us
Company
Newsroom
Quick links
Extranet
Select site
Search
Follow SSAB
Brands
Strenx
Hardox
Docol
GreenCoat
Toolox
Armox
Duroxite
SSAB Boron
SSAB Domex
SSAB Form
SSAB Laser
SSAB Weathering
SSAB Multisteel
COR-TEN
Products
Industries
Steel categories
Strenx overview
Product offer and datasheets
Products
Strenx for trailers
Strenx for agriculture
Customer cases
Strenx guarantee
Download
In focus
My Inner Strenx
Contact Strenx
Sales
Tech support
Follow Strenx
Strenx 1300 E/F
Strenx 1100
Strenx 960
Strenx 900
Strenx 700
Strenx 650
Strenx 600
Strenx 100-110
Strenx Tube
Strenx sections
Strenx 1100 Product Group
Strenx 1100 E/F
Strenx 1100 Plus
Strenx 1100MC
Strenx 1100 CR
Strenx 960 E/F
Strenx 960MC
Strenx 960 Plus
Strenx 960 CR
Strenx 900 E/F
Strenx 900MC
Strenx 900 Plus
Strenx 700 Product Group
Strenx 700 E/F
Strenx 700MC D/E
Strenx 700MC Plus
Strenx 700 CR
Strenx 700 OME
Strenx P700
Strenx 650MC D/E
Strenx 600MC D/E
Strenx 110 XF
Strenx 100
Strenx 100 XF
Strenx Tube 700MH
Strenx Tube 700MLH
Strenx Tube 700QLH
Strenx Tube 900MH
Strenx Tube 960MH
Strenx Tube 960QLH
Support excellence
Certified agricultural equipment
Certified lifting equipment
Certified trailers
Videos
Hardox overview
Product program and datasheets
Products
Customer cases
Download
In focus
Hardox In My Body
Contact Hardox
Sales
Tech support
Follow Hardox
Hardox HiAce
Hardox HiTuf
Hardox 400
Hardox 450
Hardox 500
Hardox 500 Tuf
Hardox 550
Hardox 600
Hardox Extreme
Hardox Round Bars
Hardox Tubes and Pipes
Hardox HiTemp
The sign of quality
Certified agricultural equipment
Certified waste & recycling equipment
Certified buckets
Certified tipper bodies
Videos
Docol overview
Automotive steel grades
Products
Applications
Resources
Download
In focus
Life Cycle Assessments
Automotive insights
Contact Docol
Sales
Tech Support
Follow Docol
Martensitic
Complex Phase
High Edge Ductility
Dual Phase with high formability
Dual Phase
Ferritic Bainitic
Press Hardening Steel
High Strength Low Alloy
Tubes
Coatings
Custom AHSS for automotive OEMs
All Martensitic Steel
Docol 900M
Docol 1100M
Docol 1200M
Docol 1300M
Docol 1400M
Docol 1500M
Docol 1700M
Docol 600CP
Docol 800CP
Docol 1000CP
Docol 1200CP
All High Edge Ductility steels
Docol 355HE
Docol 420HE
Docol 460HE
Docol 500HE
All Dual Phase with high formability
Docol 600DH
Docol 800DH
Docol 500DP
Docol 600DP
Docol 800DP
Docol 1000DP
Docol PHS 1500
Docol PHS 1800
Docol PHS 2000
Docol 420LA
Docol 460LA
Docol 500LA
Docol 550LA
Docol 600LA
Docol 650LA
Docol 700LA
Docol 800LA
Docol Tube 420LA
Docol Tube 500LA
Docol Tube 600LA
Docol Tube 700LA
Docol Tube R8
Docol Tube 590DP
Docol Tube 780DP
Docol Tube 980DP
Galfan
Galvannealed
Zinc
Recommended steel grades
Docol in bumpers
Docol in chassis
Docol in door beams
Docol in body-in-white
Docol in racing
Docol EV design concept
Automotive steel resources
Trial material stock
AHSS/UHSS webinars
AHSS/UHSS welding handbook
Automotive Insights blog
AHSS forming data
GreenCoat overview
10 good reasons
Why color coated steel
Colors
Download
Products
GreenCoat products
Other color coated products
In focus
Award-winning architecture
Sustainability
BIMobject
GreenCoat Partner
Contact GreenCoat
Sales
Tech Support
Follow GreenCoat
By function
By segment
By product name
Roofing
Facades
Rainwater systems
Roofing
Facades
Rainwater systems
Indoor applications
GreenCoat Cool
GreenCoat Crown BT
GreenCoat FoodSafe BT
GreenCoat Hiarc
GreenCoat Hiarc Max
GreenCoat Mica BT
GreenCoat PLX
GreenCoat Pural BT
GreenCoat Pural Farm BT
GreenCoat Pro BT
GreenCoat RWS
GreenCoat PLX – overview
GreenCoat PLX Legacy
GreenCoat PLX Pro BT
GreenCoat PLX Pural BT
Epoxy
Laminate FoodSafe
Nova
P200
Polyester
Polyester Indoor
Rough Matt Polyester
Toolox overview
Product offer and datasheets
Products
Download
In focus
Distributors
Customer cases
Contact Toolox
Sales
Tech Support
Follow Toolox
Toolox 33
Toolox 40
Toolox 44
Toolox 33 Round Bars
Toolox 44 Round Bars
Armox overview
Armor steel
Product offer and datasheets
Download
Products
Armox 370T Class 1
Armox 370T Class 2
Armox 440T
Armox 500T
Armox 600T
Armox Advance
Ramor
Contact Armox
Sales
Tech Support
Follow Armox
Ramor 300
Ramor 400
Ramor 450
Ramor 500
Ramor 550
Ramor 600
Duroxite
Products
Plate
Pipe
Pin
Welding consumables
Download
Brochure & Data Sheets
Contact Duroxite
Ask Us
Sales
Tech support
Follow Duroxite
Duroxite 100
Duroxite 101
Duroxite 200
Duroxite 201
Duroxite 300
Duroxite 500
Duroxite 100 Pipe
Duroxite 400
Duroxite 100 Wire
Duroxite 200 Wire
Duroxite AP Wire
Duroxite AP Electrode
Duroxite Cr-Zero Wire
SSAB Boron overview
About SSAB Boron
Download
In focus
SSAB M43
Products
Product offer and datasheets
Hot rolled
Cold rolled
SSAB Boron Tube 22
Contact SSAB Boron
Sales
Tech Support
SSAB Boron 22
SSAB Boron 24
SSAB Boron 27
SSAB Boron 27Cr
SSAB Boron 30
SSAB Boron 33
SSAB Boron 33Cr
SSAB Boron 36
SSAB Boron 38
SSAB Boron 42
SSAB Boron 22
SSAB Boron 27Cr
SSAB Boron 38
SSAB Domex overview
Download
In focus
SSAB Domex Plus
Products
Product offer and datasheets
Hot rolled
Cold rolled
Metal coated
Tubes
SSAB Domex sections
Contact SSAB Domex
Sales
Tech Support
SSAB Domex 315MC
SSAB Domex 355MC
SSAB Domex 420MC
SSAB Domex 460MC
SSAB Domex 500MC
SSAB Domex 550MC
SSAB Domex 355MC Plus
SSAB Domex 420MC Plus
SSAB Domex 460MC Plus
SSAB Domex 500MC Plus
SSAB Domex 240YP
SSAB Domex 355ML
SSAB Domex 420ML
SSAB Domex 460ML
SSAB Domex 500ML
SSAB Domex 220LA
SSAB Domex 260LA
SSAB Domex 280LA
SSAB Domex 300LA
SSAB Domex 340LA
SSAB Domex 350LA
SSAB Domex 380LA
SSAB Domex 420LA
SSAB Domex 460LA
SSAB Domex 500LA
Metal coated HSLA steels
Metal coated structural steels
SSAB Domex Tube 235 JRH
SSAB Domex Tube 355 J2H
SSAB Domex Tube 460MH
SSAB Domex Tube 500MH
SSAB Domex Tube 550MH
SSAB Domex Tube Double Grade
SSAB Form overview
Download
Products
Product offer and datasheets
Hot rolled
Cold rolled
Metal coated formable steels
Tubes
Contact SSAB Form
Sales
Tech Support
SSAB Form 200 HR
SSAB Form 200 CR
SSAB Form 03
SSAB Form 04
SSAB Form 05
SSAB Form 06
SSAB Form 07
SSAB Form Tube 190
SSAB Form Tube 220
SSAB Form Tube 220 Plus
SSAB Form Tube 320
SSAB Form Tube 420
SSAB Form Tube 420 Plus
SSAB Laser overview
Download
Products
Product offer and datasheets
Hot rolled plate
Hot rolled sheet
Cold rolled sheet
In focus
Distribution partners
Contact SSAB Laser
Sales
Tech Support
SSAB Laser 250C
SSAB Laser 275C
SSAB Laser 355C
SSAB Laser 355ML Plus
SSAB Laser 420ML Plus
SSAB Laser 460ML Plus
SSAB Laser 250C
SSAB Laser 275C
SSAB Laser 355C
SSAB Laser 355MC Plus
SSAB Laser 420MC Plus
SSAB Laser 460MC Plus
SSAB Laser DC03
SSAB Weathering
Download
Products
Product offer and datasheets
Hot rolled
Cold rolled
Tubes
SSAB Weathering sections
In focus
Buildings
Heavy transport
Structures and bridges
Processing industries
Contact SSAB Weathering
Sales
Tech Support
COR-TEN
SSAB Weathering 355
SSAB Weathering 420M ML
SSAB Weathering 460M ML
SSAB Weathering 550
SSAB Weathering 700
SSAB Weathering 960
COR TEN A for facades
COR-TEN
SSAB Weathering 355
SSAB Weathering 700
SSAB Weathering Tube 355WH
SSAB Weathering Tube 500WH
COR-TEN B Tube
SSAB Multisteel overview
Product offer and datasheets
Hot rolled
SSAB Multisteel HS
SSAB Multisteel PA
SSAB Multisteel PE
SSAB Multisteel PEA
SSAB Multisteel PES
SSAB Multisteel SN
SSAB Multisteel SNL
Contact SSAB Multisteel
Sales
Tech Support
COR-TEN overview
Download
Products
Product offer and datasheets
Hot rolled
Cold rolled
COR-TEN A for façades
Tubes
Contact COR-TEN
Sales
Tech Support
Automotive
Building industry
Offshore marine energy
Lifting
Infrastructure solutions
Transportation
Yellow goods and construction machinery
Raw material handling
Wear-resistant steels
Structural and cold forming steels
Metal coated coils and sheets
Color coated coils and sheets
Overlay products
Hollow sections
Open sections
Precision tubes
Steel piles and infrastructure products
Wear-resistant steels
Wear plates
Boron
Tubes & pipes
Round bars
Overlay products
Hardox Hi-Tuf
Hardox 400
Hardox 450
Hardox 500
Hardox 500 Tuf
Hardox 550
Hardox 600
Hardox Extreme
Hardox Hi-Temp
SSAB Boron 22
SSAB Boron 24
SSAB Boron 27
SSAB Boron 27Cr
SSAB Boron 30
SSAB Boron 33
SSAB Boron 33Cr
SSAB Boron 36
SSAB Boron 38
SSAB Boron 42
Hardox tubes and pipes
SSAB Boron Tube 22
Hardox Round Bars
Duroxite 100
Duroxite 100 Pipe
Duroxite 100 Wire
Duroxite 101
Duroxite 200
Duroxite 200 Wire
Duroxite 201
Duroxite 300
Duroxite 400
Duroxite 500
Structural and cold forming steels
Strenx
Docol
SSAB Domex
SSAB Laser
SSAB Weathering and COR-TEN
Pole sheet
Metal coated
Strenx 100
Strenx 100 XF
Strenx 110 XF
Strenx 600MC
Strenx 650MC
Strenx 700
Strenx 700MC
Strenx 700MC Plus
Strenx 700 CR
Strenx 700 OME
Strenx 900
Strenx 900 Plus
Strenx 900MC
Strenx 960
Strenx 960 Plus
Strenx 960MC
Strenx 960 CR
Strenx 1100
Strenx 1100 Plus
Strenx 1100MC
Strenx 1100 CR
Strenx 1300
3rd generation steel
Docol 420LA
Docol 460LA
Docol 500LA
Docol 550LA
Docol 600LA
Docol 650LA
Docol 700LA
Docol 800LA
Docol 500DP
Docol 600DP
Docol 800DP
Docol 1000DP
Docol 600CP
Docol 800CP
Docol 1000CP
Docol 1200CP
Docol 900M
Docol 1100M
Docol 1200M
Docol 1300M
Docol 1400M
Docol 1500M
Docol 1700M
Docol PHS 1500
Docol PHS 1800
Docol PHS 2000
Docol 600FB
SSAB Domex 220LA
SSAB Domex 240YP
SSAB Domex 260LA
SSAB Domex 280LA
SSAB Domex 300LA
SSAB Domex 315MC
SSAB Domex 340LA
SSAB Domex 350LA
SSAB Domex 355MC
SSAB Domex 355MC Plus
SSAB Domex 355ML
SSAB Domex 380LA
SSAB Domex 420LA
SSAB Domex 420MC
SSAB Domex 420MC Plus
SSAB Domex 420ML
SSAB Domex 460LA
SSAB Domex 460MC
SSAB Domex 460MC Plus
SSAB Domex 460ML
SSAB Domex 500LA
SSAB Domex 500MC
SSAB Domex 500MC Plus
SSAB Domex 500ML
SSAB Domex 550MC
SSAB Laser 250C
SSAB Laser 275C
SSAB Laser 355C
SSAB Laser 355ML Plus
SSAB Laser 420ML Plus
SSAB Laser 460ML Plus
SSAB Laser 355MC Plus
SSAB Laser 420MC Plus
SSAB Laser 460MC Plus
SSAB Laser DC03
COR-TEN
SSAB Weathering 355
SSAB Weathering 550
SSAB Weathering 700
SSAB Domex MC HSLA
SSAB Domex MC structural steels
SSAB Form metal coated
Metal coated coils and sheets
HSLA steels
Structural steels
Formable steels
Automotive AHSS & HSLA steels
Coatings
Metal coated HSLA steels
Metal coated structural steels
SSAB Form 200
SSAB Form 52
SSAB Form 53
SSAB Form 54
SSAB Form 56
SSAB Form TSP
Docol 420LA
Docol 460LA
Docol 550LA
Docol 700LA
Docol 500DP
Docol 600DP
Docol 800DP
Docol 600CP
Docol 800CP
Docol 1000CP
Zinc coating
Galfan coating
Galvannealed coating
Overlay products
Duroxite
Hollow sections
Product offer and datasheets
Strenx Tube
SSAB Domex Tubes
SSAB Weathering Tube
Contact Hollow Sections
Sales
Tech support
Strenx Tube 700MH
Strenx Tube 700MLH
Strenx Tube 700QLH
Strenx Tube 900MH
Strenx Tube 960MH
Strenx Tube 960QLH
SSAB Domex Tube 235 JRH
SSAB Domex Tube 355 J2H
SSAB Domex Tube Double Grade
SSAB Domex Tube 460MH
SSAB Domex Tube 500MH
SSAB Domex Tube 550MH
SSAB Weathering Tube 355WH
SSAB Weathering Tube 500WH
COR-TEN B Tube
Open sections
Product offer and datasheets
SSAB Domex Sections
SSAB Weathering Sections
Strenx Sections
Contact Open sections
Sales
Tech support
Precision tubes
Product offer and datasheets
Docol Tube
SSAB Form Tube
SSAB Boron Tube
Contact Precision tubes
Sales
Tech support
Docol Tube 420LA
Docol Tube 500LA
Docol Tube 600LA
Docol Tube 700LA
Docol Tube 590DP
Docol Tube 780DP
Docol Tube 980DP
Docol Tube R8
SSAB Form Tube 190
SSAB Form Tube 220
SSAB Form Tube 220 Plus
SSAB Form Tube 320
SSAB Form Tube 420
SSAB Form Tube 420 Plus
SSAB Boron Tube 22
Steel piles and infrastructure products
Product offer and datasheets
Products
Steel piles
Retaining walls
Safety barriers
Pressure pipes
Trapezoidal sections
Expandable Rock Bolts
In focus
Customer cases
Downloads
News archive
Contact Steel piles and infrastructure products
Sales
Tech support
Micropiles
Large diameter piles
RD casings
Combi wall
RD pile wall
Water mains
Spirally welded pipes
Support
Webinar center
Processing
Design and development support
Calculators and tools
Orders and deliveries
Challenge
Handbooks
Product Data Matrix Marking
Service offers
Parts & kits
Engineering services
Processing services
SSAB Shape
Service centers
Hardox Wearparts
About SSAB
Careers
Investors
Sustainability
About SSAB
SSAB in brief
Our business
Operating environment
Strategy
Management
Contractors and suppliers
Swedish Steel Prize
SSAB in brief
Vision and values
SSAB story
History
Corporate identity and brands
ABC of steel
Our business
SSAB Special Steels
SSAB Europe
SSAB Americas
Tibnor
Ruukki Construction
Sites all over the world
Research and development
How we work with customers
Operating environment
Steel market and SSAB’s position
SSAB's customer segments
Global megatrends affecting SSAB
Strategy
SSAB's value chain
Taking the Lead -strategy
Management
Board of directors
Group Executive Committee
Careers
Job opportunities
Why SSAB
Working at SSAB
Meet our people
Students
Why SSAB
Diversity and equal opportunities
Health and safety
Leadership at SSAB
Working at SSAB
Develop with SSAB
High performing organization
Young professionals
Students
Thesis and internship opportunities
Investors
SSAB as an investment
SSAB share
Reports and presentations
Financial information
Debt financing
Corporate governance
IR calendar
IR contacts
SSAB as an investment
SSAB fact sheet
Financial targets
Market situation and outlook
Operating environment
Strategy
Acquisitions and divestments
Analysts
Consensus estimates
Rautaruukki financial reports
Share information
Share monitor
Share capital
Share related key figures
Dividend
Closing price history
Investment calculator
Shareholders
Alternative exchanges
Flagging notifications
Key figures
Reporting schedule and segments
Definition of key figures
Annual and quarterly financials tool
Financial risks
Sensitivity analysis
Corporate governance
General meetings
Board of Directors
Group Executive Committee
Audit Committee
Remuneration Committee
Nomination Committee
Internal audit
External auditors
Internal control
Remuneration
Remuneration to senior executives
Corporate governance reports
Articles of association
Sustainability
Our sustainability approach
First in fossil-free steel
Leading sustainability performance
Documents
Our sustainability approach
Sustainability strategy
Sustainability targets 2020
Sustainability targets beyond 2020
SSAB's value chain
Sustainability performance
UN Sustainable development goals
Sustainability governance
Stakeholders
Materiality analysis
First in fossil-free steel
Use better steel: SSAB’s customers benefit from leading CO₂ efficient production
Use steel better: Environmental benefits with SSAB's steels
Go fossil-free: First in fossil-free steel
Use steel better: Environmental benefits with SSAB's steels
EcoUpgraded concept
SSAB in the circular economy
Steel life cycle
Sustainability and high-strength steels
Sustainable construction solutions
External sales of by products
Leading sustainability performance
Safety first
Resource efficient operations
Responsible sourcing
Zero tolerance for bribery and corruption
High-performing organization
SSAB in the community
Resource efficient operations
Steel production
Energy efficiency
Material efficiency
Newsroom
Media archive
Images and videos
SSAB in social media
Subscribe and order
Media contacts
Contact SSAB
Sales
Questions about products and services
Contact sales
Tech Support
Deep knowledge and years of experience
Contact Tech support
Find your SSAB contacts
Contact us
International
International (English)
Africa
South Africa (English)
America
Brasil (Português)
Canada (English)
Latinoamérica (Español)
USA (English)
Asia
中国 (中文)
日本語 (日本語)
한국어 (한국어)
Europe
Czech (Čeština)
España (Español)
Français (Français)
Deutschland (Deutsch)
Magyarország (Magyar)
Italia (Italiano)
Nederland (Engels)
Polska (Polski)
Romania (Română)
Россия (Русский)
Suomi (Suomi)
Sverige (Svenska)
Türkçe (Türkçe)
U.K. (English)
Suggested searches
Brands & products
Hardox
Download
Share this:
Download
Hardox® 400 Round bar turning recommendations
799 Kb
Hardox® 400 Rundstähle – Drehempfehlungen
145 Kb
English
Deutsch
Hardox® 400 Round bar band sawing recommendations
255 Kb
Hardox® 400 Rundstähle – Bandsägeempfehlungen
160 Kb
English
Deutsch
Hardox® wear plate – The Beast
8,22 Mb
Hardox® wear plate – Das Biest
7,07 Mb
Hardox® wear plate – La Bestia
15,64 Mb
Hardox® wear plate – La bête
7,12 Mb
Hardox® wear plate – La Bestia
6,97 Mb
Hardox 경도와 인성의 최적 조합
66,55 Mb
Trudnościeralna blacha Hardox® - Bestia
27,57 Mb
Hardox® wear plate – Dureza e Resistência
7,34 Mb
Нам нет износа
26,89 Mb
Hardox® wear plate – The Beast
7,36 Mb
ความแข็ง และความ เหนยีว
4,72 Mb
Hardox® aşınma plakası – Sert ve Tok
8,74 Mb
QUÁI THÚ
32,14 Mb
野兽是我
3,49 Mb
English
Deutsch
Español (España)
Français
Italiano
한국어
Polski
Português (Brasil)
Русский
Svenska
ไทย
Türkçe
Tiếng việt
中文
TechSupport #55: Upgrading from Hardox® 400 to Hardox® 450
1,09 Mb
Techsupport Nr. 55 Upgrade von Hardox® 400 auf Hardox® 450
1,08 Mb
TechSupport #55: Passare da Hardox® 400 a Hardox® 450
1,09 Mb
Upgrading from Hardox 400 to Hardox 450
1,22 Mb
TECHSUPPORT #55 从 Hardox 400 升级到 Hardox 450
327 Kb
English
Deutsch
Italiano
Русский
中文
Hardox® 500 Tuf for recycling containers
2,0 Mb
Hardox® 500 Tuf für Recyclingbehälter
2,4 Mb
Hardox® 500 Tuf for recycling containers
2,15 Mb
Hardox® 500 Tuf pour les containers de recyclage
2,36 Mb
Hardox® 500 Tuf - La nuova generazione Hardox® per container
2,39 Mb
自卸车车体专用 新一代Hardox®悍达耐磨钢
4,92 Mb
English
Deutsch
Suomi
Français
Italiano
中文
The Workshop properties for Hardox® 400 round bar
269 Kb
Bearbeitungshinweise für Hardox® 400 Rundstähle
190 Kb
English
Deutsch
Hardox® in My Body - The Sign of Quality
4,29 Mb
Garantia de calidad - Hardox® In My Body
4,08 Mb
Laadun merkki - Hardox® In My Body
5,0 Mb
Hardox® in My Body - Symbol jakości
4,15 Mb
A marca da qualidade - Hardox® In My Body
3,91 Mb
Hardox® In My Body - Знак качества
3,9 Mb
Hardox® in My Body - The sign of quality
4,29 Mb
English
Español (España)
Suomi
Polski
Português (Brasil)
Русский
Türkçe
Hardox® 500 Tuf for tipper bodies
2,12 Mb
Hardox® 500 Tuf für Kipper
2,09 Mb
Hardox® 500 Tuf informatión - volquete
2,41 Mb
Hardox® 500 Tuf information - tipper
2,15 Mb
Hardox® 500 Tuf pour les bennes
2,09 Mb
Hardox® 500 Tuf – La nuova generazione Hardox® per cassoni
2,11 Mb
Информация о стали Hardox® 500 Tuf
2,17 Mb
Hardox® 500 Tuf information
2,16 Mb
自卸车车体专用 新一代Hardox®悍达耐磨钢
3,14 Mb
English
Deutsch
Español (España)
Suomi
Français
Italiano
Русский
Türkçe
中文
Hardox® 500 Tuf for buckets
1,94 Mb
Hardox® 500 Tuf für Schaufeln
1,91 Mb
Hardox® 500 Tuf for buckets
1,92 Mb
Hardox® 500 Tuf pour les godets
1,94 Mb
Hardox® 500 Tuf - La nuova generazione Hardox® per benne
1,94 Mb
铲斗专用 新一代 Hardox® 悍达耐磨钢
4,79 Mb
English
Deutsch
Suomi
Français
Italiano
中文
Hardox® HiTemp can take the heat
2,63 Mb
Hardox® HiTemp für hohe Temperaturen
2,64 Mb
Hardox® HiTemp Kestää Kuumuutta
2,64 Mb
Hardox® HiTemp résiste aux températures élevées
1,98 Mb
Hardox® HiTemp resiste al caldo
2,64 Mb
熱に強いHardox® HiTemp (ハルドックス・ハイテンプ)
2,8 Mb
Hardox® HiTemp lubi, gdy jest gorąco
2,7 Mb
Жаропрочная сталь Hardox® HiTemp
2,72 Mb
Hardox® HiTemp för heta miljöer
2,64 Mb
Hardox® HiTemp 耐高温型悍达钢
2,88 Mb
English
Deutsch
Suomi
Français
Italiano
日本語
Polski
Русский
Svenska
中文
Hardox® Onsite - Road building
1,38 Mb
Hardox® na mjestu primjene Cestogradnja
3,03 Mb
Hardox® w terenie - budowa dróg
1,38 Mb
Hardox®悍达钢的应用 筑路行业 臺通往成功的重要一步
11,35 Mb
English
Hrvatski
Polski
中文
Hardox® Onsite - Recyling
1,37 Mb
Hardox® a pie de obra Reciclaje
1,38 Mb
Hardox® w terenie - recykling
2,06 Mb
Hardox® 在现场 回收利用 您通往成功的重要一步
1,76 Mb
English
Español (España)
Polski
中文
Hardox® Onsite - Quarry & open pit mining
0,99 Mb
Hardox® a pie de obra - Canteras y minería a cielo abierto
1,01 Mb
Hardox® na mjestu primjenekamenolom i površinski kop
2,63 Mb
Hardox® w terenie - kamieniołomy i kopalnie odkrywkowe
1,46 Mb
HARDOX ในการท างานจรงิ เหมอืงหนิและเหมอืงแรแ่บบเปิด
969 Kb
Hardox® Taş Ocağı ve Açık Maden Ocağı Broşürü
1,42 Mb
HARDOX TRÊN CÔNG TRƯỜNG Mỏ Đá & Mỏ Lộ Thiên
2,16 Mb
Hardox®悍达钢的应用 采石场和露天矿 您通往成功的重要一步
11,15 Mb
English
Español (España)
Hrvatski
Polski
ไทย
Türkçe
Tiếng việt
中文
Hardox® Onsite - Underground mine
674 Kb
Hardox® na mjestu primjenepodzemni rudnik
2,4 Mb
Hardox® w terenie - górnictwo podziemne
1,2 Mb
Hardox®悍达钢的应用 地下矿井 您通往成功的重要一步
10,87 Mb
English
Hrvatski
Polski
中文
Hardox® Onsite - Cement
4,89 Mb
Hardox® - Cemento in situ
9,24 Mb
Hardox® na mjestu primjene - Cement
5,07 Mb
HARDOX TRÊN CÔNG TRƯỜNG XI MĂNG
7,02 Mb
现场应用水泥
3,38 Mb
English
Español (España)
Hrvatski
Tiếng việt
中文
Hardox® guarantees
4,41 Mb
English
Welding of Hardox®
6,99 Mb
Schweissen von Hardox®
7,04 Mb
Soldadura Hardox®
2,05 Mb
Hitsaus Hardox®
3,28 Mb
Soudage Hardox®
7,09 Mb
A Hardox® Acél Hegesztése
7,21 Mb
Saldatura Hardox®
7,05 Mb
Hardox 제품의 용접
7,09 Mb
Spawanie blachy Hardox®
7,16 Mb
Soldagem Hardox®
6,99 Mb
Сварка Hardox®
717 Kb
Svetsning av Hardox®
3,0 Mb
Hardox 悍达钢焊接指导手册
801 Kb
English
Deutsch
Español (España)
Suomi
Français
Magyar
Italiano
한국어
Polski
Português (Brasil)
Русский
Svenska
中文
Product program - Hardox®, Strenx® and Toolox® - imperial
278 Kb
English
Product program - Hardox ®, Strenx ® and Toolox ® - metric
244 Kb
Product program - Hardox ®, Strenx ® and Toolox ®
321 Kb
English
Русский
Thermal cutting of Hardox® and Strenx®
1,32 Mb
Thermisches Schneiden von Hardox® und Strenx®
630 Kb
Cięcie termiczne stali Hardox® i Strenx®
318 Kb
Corte térmico de Hardox® e Strenx®
279 Kb
Thermal cutting of Hardox® and Strenx®
536 Kb
技术支持 #16 Hardox 和 Strenx 系列钢材的热切割
4,66 Mb
English
Deutsch
Polski
Português (Brasil)
Русский
中文
Bending of high strength steel - Strenx®, Hardox®, Docol®
337 Kb
Gięcie stali o wysokiej wytrzymałości - Strenx®, Hardox®, Docol®
394 Kb
Bending of high strength steel - Strenx®, Hardox®, Docol®
415 Kb
Strenx®, Hardox® 和 Docolx® - 高强度钢材折弯指导手册
12,64 Mb
English
Polski
Русский
中文
TechSupport #29: Welding of cutting edge to bucket/ adapters to cutting edge - Hardox®
987 Kb
English
Hardox Wearparts® your one stop wear shop
31,43 Mb
Hardox Wearparts® ihr one stop shop rund um den verschleiß
20,18 Mb
Hardox Wearparts® su solución para combatir el desgaste
5,83 Mb
Hardox Wearparts® - one stop wear shop
42,74 Mb
Hardox Wearparts® votre guichet unique pour les pièces d'usure
6,43 Mb
Hardox Wearparts® - wszystkie części w jednym miejscu
20,33 Mb
Hardox Wearparts® butik för slitdelsprodukter
36,61 Mb
Hardox Wearparts® - aşinma ürünlerİ İçİn tek adresİnİz
6,55 Mb
您的一站式耐磨商店
48,95 Mb
English
Deutsch
Español (España)
Suomi
Français
Polski
Svenska
Türkçe
中文
SSAB Product and delivery information - Oxelösund Site
452 Kb
English
40 years of wear and still loving it - Hardox®
4,8 Mb
Dopo 40 anni, Hardox® è più duro e tenace che mai
8,76 Mb
Нам нет износа уже 40 лет, и это только начало
4,99 Mb
English
Italiano
Русский
General product information - Strenx® , Hardox®, Armox®, Toolox®
2,73 Mb
Общая информация о продукции - Strenx®, Hardox®, Armox®, Toolox®
299 Kb
产品信息手册 Strenx钢、Hardox悍达钢、 Armox铠达钢和 Toolox拓达钢
2,35 Mb
English
Русский
中文
Hardox® pipes and tubes - the inside story
1,94 Mb
English
Hardox round bars for rod mills
3,72 Mb
Hardox® Rundstäbe für Stabrohrmühlen
3,73 Mb
English
Deutsch
Hardox® 400 round bars - The shape of excellence
4,81 Mb
Hardox 400 Rundstahl - Formvollendete Höchstleistung
4,81 Mb
English
Deutsch
Hardox® HiAce for acid environments
1,2 Mb
산성 환경을 위한 HARDOX® HiACE 소개
1,37 Mb
English
한국어
Kelly Attachments relies on Hardox® round bars for quick couplers
1,05 Mb
English
SSAB AR 500 Round bar
245 Kb
English