Armox protection plate

Armox® 500T

High hardness armor with extrordinary toughness properties.

Armox® 500T is the world’s toughest protection plate, having nominal 500 HBW hardness, for use in vehicles, buildings and many more applications.

Benefits of Armox® 500T include:

  • Market-leading steel protection
  • Superior workshop properties
  • Optimized solutions
  • Perfect hardness/toughness balance, for combined penetration and blast protection
  • Expertise in ballistic protection from SSAB

It offers vehicle designers new ways to increase protection using lighter weight designs. 

Armox® 500T is not intended for further heat treatment.

Dimension range

Armox® 500T is available in thicknesses between 3.0 and 80.0 mm. Other dimensions to be agreed with SSAB.

Available Standards

EN 10029

Armox 500T

Armox 500T

USED FOR
DIMENSIONS
STANDARDS
DATA SHEET
USED FOR

Armored

DIMENSIONS

T: 3 - 80 mm

STANDARDS

EN 10029

DATA SHEET