How to weld > Welding thermal cycle

Recommended t₈⸝₅values

If the t₈⸝₅ value for a certain welding situation is not calculated, appropriate t₈⸝₅ values are automatically attained if all other welding recommendations are followed.

If the t8/5 value for a certain welding situation is not calculated, appropriate t8/5 values are automatically attained if all other welding recommendations are followed. Improper t8/5 values can result in:

  • Impaired impact toughness throughout the joint compared to welding within the recommended t8/5 range. Lowered toughness values can occur for both too high and too low values of t8/5.
  • Too high t8/5 values outside the recommendations may contribute to reduced static strength in the joint and a wider soft zone in the HAZ.

The recommended t8/5 values from SSAB are mostly emphasized for welding of the Strenx® grades. Both normal as well as optimized conditions for mechanical properties in welded structures are presented.

For the Hardox® grades the recommended t8/5 values are less emphasized compared to welding of Strenx® in many situations. The reasons are that there are normally less requirement with respect to impact toughness and static strength in joints of these structures. However recommended t8/5 values exists. These intervals depends both of the Hardox® grade and its plate thickness range. These values can be found in SSAB WeldCalc.

Contact Technical support


The information in this report is only applicable to SSAB’s products and should not be applied to any other products than original SSAB products. 


This report provides general results and recommendations for SSAB steel products. This report is subject to SSAB’s Terms of Use. It shall be the user's responsibility to verify that the information contained herein is correct and is suitable to be used for the particular purpose and application of the user. The report is intended to be used by professional users only who possess adequate expertise, qualification and knowledge for the safe and correct use of the results and recommendations in this report. This report is provided “as is”. The use of the report is at user’s own discretion and risk and that users will be solely responsible for any use of this report. SSAB disclaims any liability for the content or potential errors of this report, including but not limited to warranties and condition of merchantability or fitness for a particular purpose or suitability for individual applications. SSAB shall not be liable for any kind of direct or indirect damages and/or costs related to or arising therefrom, whether special, incidental, consequential or directly or indirectly related to the use of, or the inability to use, the report or the content, information or results included therein. 