How to weld > Welding thermal cycle

The t₈⸝₅ value

The thermal cycle of welding can be defined by the cooling time in the HAZ between +800°C and +500°C.

This parameter is called the t8/5 value. It is illustrated in the graph below.

Schematic diagram for a thermal heat treatment in the part of the HAZ situated closest to the weld metal.

There is no need to calculate the t8/5 value. However, it facilitates a good understanding of the thermal treatment in the joint.

The t8/5 value is mainly calculated. Evaluations of the t8/5 value show that it is close to constant throughout different parts of the joint. That is true as long as the peak temperature in the joint reaches above +900°C during the welding performance.

The formulas for the calculation of the t8/5 value is explained in the SSAB Welding Handbook.

Contact Technical support


The information in this report is only applicable to SSAB’s products and should not be applied to any other products than original SSAB products. 


This report provides general results and recommendations for SSAB steel products. This report is subject to SSAB’s Terms of Use. It shall be the user's responsibility to verify that the information contained herein is correct and is suitable to be used for the particular purpose and application of the user. The report is intended to be used by professional users only who possess adequate expertise, qualification and knowledge for the safe and correct use of the results and recommendations in this report. This report is provided “as is”. The use of the report is at user’s own discretion and risk and that users will be solely responsible for any use of this report. SSAB disclaims any liability for the content or potential errors of this report, including but not limited to warranties and condition of merchantability or fitness for a particular purpose or suitability for individual applications. SSAB shall not be liable for any kind of direct or indirect damages and/or costs related to or arising therefrom, whether special, incidental, consequential or directly or indirectly related to the use of, or the inability to use, the report or the content, information or results included therein.