How to weld > Welding thermal cycle

The outcome of the thermal cycle

The characteristics of the thermal heat treatment from welding are of crucial importance for the mechanical properties and the microstructures in the HAZ.

Its outcome depends primarily on:

  • The level of the heat input  
  • The plate thickness in the joint
  • The type of joint
  • The preheat temperature, if applicable.

As an example, the thermal cycles during a welding performance, at different locations in the joint, are illustrated below.

The heating and cooling rate and the peak temperature decrease with increased distance to the arc.

Contact Technical support


The information in this report is only applicable to SSAB’s products and should not be applied to any other products than original SSAB products. 


This report provides general results and recommendations for SSAB steel products. This report is subject to SSAB’s Terms of Use. It shall be the user's responsibility to verify that the information contained herein is correct and is suitable to be used for the particular purpose and application of the user. The report is intended to be used by professional users only who possess adequate expertise, qualification and knowledge for the safe and correct use of the results and recommendations in this report. This report is provided “as is”. The use of the report is at user’s own discretion and risk and that users will be solely responsible for any use of this report. SSAB disclaims any liability for the content or potential errors of this report, including but not limited to warranties and condition of merchantability or fitness for a particular purpose or suitability for individual applications. SSAB shall not be liable for any kind of direct or indirect damages and/or costs related to or arising therefrom, whether special, incidental, consequential or directly or indirectly related to the use of, or the inability to use, the report or the content, information or results included therein. 

Copyright 2026