How to weld > Welding consumables

Examples of suitable MAG solid wires

The consumables are arranged according to the yield strength (Rₚ₀.₂) for which they are classified. In reality, a given consumable normally has a higher yield strength than its standard designation. The mechanical properties of a given consumable can be obtained from its manufacturer.
Consumable manufacturer/ Min yield strength MPa (ksi)
Consumable manufacturer/ Min yield strength MPa (ksi)
AWS Class
400 (58)
ER 70X*
470 (68)
ER 80X*
540 (78)
ER 90X*
610 (97)
CM2-IGER100X*
680 (100)
ER110X*
745 (108)
ER120X*
Consumable manufacturer/ Min yield strength MPa (ksi)
Consumable manufacturer/ Min yield strength MPa (ksi)
ELGA
400 (58)
Elgamatic 100
470 (68)
Elgamatic 162
540 (78)
Elgamatic 163
610 (97)
Elgamatic 135
680 (100)
745 (108)
Elgamatic 138
Consumable manufacturer/ Min yield strength MPa (ksi)
Consumable manufacturer/ Min yield strength MPa (ksi)
ESAB
400 (58)
OK Aristorod 12.50, OK Aristorod 12.63
470 (68)
Elgamatic 162 OK Aristorod 13.09, OK Aristorod 13.12
540 (78)
OK Aristorod 13.22 
610 (97)
OK Aristorod 55, OK Autrod 13.25
680 (100)
OK Aristorod 69
745 (108)
OK Aristorod 79
Consumable manufacturer/ Min yield strength MPa (ksi)
Consumable manufacturer/ Min yield strength MPa (ksi)
LINCOLN ELECTRIC
400 (58)
LNM 25, SUPRAMIG HD
470 (68)
LNM Ni1, LNM Ni2.5
540 (78)
610 (97)
LNM MoNi, Superarc AK 10-TM
680 (100)
LNM MoNiVa
745 (108)
LNM MoNiCr
Consumable manufacturer/ Min yield strength MPa (ksi)
Consumable manufacturer/ Min yield strength MPa (ksi)
BÖHLER
400 (58)
EMK6, EMK8
470 (68)
NiCu1-IG, DCMS-IG
540 (78)
CM2-IG
610 (97)
Union NiMoCr
680 (100)
X70-IG, alform 700-IG 
745 (108)
Union X90, Union X96
Consumable manufacturer/ Min yield strength MPa (ksi)
Consumable manufacturer/ Min yield strength MPa (ksi)
OERLIKON
400 (58)
Carbofil 1, Carbofil 1 Gold
470 (68)
Carbofil NiCu
540 (78)
610 (97)
Carbofil NiMoCr, Carbofil NiMo1
680 (100)
745 (108)
Carbofil 120

* X can stand for one or several code characters

Contact Technical support


The information in this report is only applicable to SSAB’s products and should not be applied to any other products than original SSAB products. 


This report provides general results and recommendations for SSAB steel products. This report is subject to SSAB’s Terms of Use. It shall be the user's responsibility to verify that the information contained herein is correct and is suitable to be used for the particular purpose and application of the user. The report is intended to be used by professional users only who possess adequate expertise, qualification and knowledge for the safe and correct use of the results and recommendations in this report. This report is provided “as is”. The use of the report is at user’s own discretion and risk and that users will be solely responsible for any use of this report. SSAB disclaims any liability for the content or potential errors of this report, including but not limited to warranties and condition of merchantability or fitness for a particular purpose or suitability for individual applications. SSAB shall not be liable for any kind of direct or indirect damages and/or costs related to or arising therefrom, whether special, incidental, consequential or directly or indirectly related to the use of, or the inability to use, the report or the content, information or results included therein. 