How to weld > Welding consumables

Examples of suitable MAG flux cored wires

The consumables are arranged according to the yield strength (Rₚ₀.₂) for which they are classified. In reality, a given consumable normally has a higher yield strength than its standard designation. The mechanical properties of a given consumable can be obtained from its manufacturer.
Consumable manufacturer/ Min yield strength MPa (ksi)
Consumable manufacturer/ Min yield strength MPa (ksi)
AWS Class
400 (58)
ER 7X*
470 (68
ER 8X”
540 (78)
ER 9X”
610 (97)
ER10X*
680 (100)
ER11X”
745 (108)
ER12X”
Consumable manufacturer/ Min yield strength MPa (ksi)
Consumable manufacturer/ Min yield strength MPa (ksi)
ELGA
400 (58)
Elgacore DWA 51B, Elgacore DWA 50
470 (68
Elgacore DWA 55L
540 (78)
Elgacore DWA 65L
610 (97)
680 (100)
Elgacore R690
745 (108)
Consumable manufacturer/ Min yield strength MPa (ksi)
Consumable manufacturer/ Min yield strength MPa (ksi)
ESAB
400 (58)
Tubrod 15.00, Filarc PZ 6113S
470 (68
OK Tubrod 15.17
540 (78)
Dual-Shield 55, Dual-Shield CrMo2
610 (97)
Dual-Shield 62
680 (100)
Dual-Shield 69, OK Tubrod 15.27
745 (108)
Filarc PZ 6149
Consumable manufacturer/ Min yield strength MPa (ksi)
Consumable manufacturer/ Min yield strength MPa (ksi)
LINCOLN ELECTRIC
400 (58)
Outershield 71E-H, Outershield 71MS-H
470 (68
Outershield 12-H, Outershield 19-H
540 (78)
Outershield 20-H
610 (97)
Outershield 101Ni-HSR
680 (100)
Outershield 690-H
745 (108)
Consumable manufacturer/ Min yield strength MPa (ksi)
Consumable manufacturer/ Min yield strength MPa (ksi)
BÖHLER
400 (58)
Ti52-FD, Union TG 55 M
470 (68
Ti 60-FD, Ti 2 Ni T-FD
540 (78)
Kb 65 T-FD
610 (97)
680 (100)
Kb 85 T-FD
745 (108)
Consumable manufacturer/ Min yield strength MPa (ksi)
Consumable manufacturer/ Min yield strength MPa (ksi)
OERLIKON
400 (58)
Fluxofil 14HD, Fluxofil 19HD
470 (68
Fluxofil 20, Fluxofil 20HD
540 (78)
610 (97)
680 (100)
745 (108)

* X can stand for one or several code characters

Contact Technical support


The information in this report is only applicable to SSAB’s products and should not be applied to any other products than original SSAB products. 


This report provides general results and recommendations for SSAB steel products. This report is subject to SSAB’s Terms of Use. It shall be the user's responsibility to verify that the information contained herein is correct and is suitable to be used for the particular purpose and application of the user. The report is intended to be used by professional users only who possess adequate expertise, qualification and knowledge for the safe and correct use of the results and recommendations in this report. This report is provided “as is”. The use of the report is at user’s own discretion and risk and that users will be solely responsible for any use of this report. SSAB disclaims any liability for the content or potential errors of this report, including but not limited to warranties and condition of merchantability or fitness for a particular purpose or suitability for individual applications. SSAB shall not be liable for any kind of direct or indirect damages and/or costs related to or arising therefrom, whether special, incidental, consequential or directly or indirectly related to the use of, or the inability to use, the report or the content, information or results included therein. 

Copyright 2026