How to weld > Shielding gas

Pulsed arc MAG welding

Welding with a pulsed arc technique means that an arc can be attained with relatively low heat inputs.

This technique uses pulsed parameters with respect to an interaction between the current and the voltage values.

The main exceptions with pulsed arc compared  to a spray arc technique are that:

  • Thinner plate thicknesses can be welded using the pulsed arc technique. Even the thinnest plate thicknesses in the Hardox and Strenx range can be welded with the pulsed arc technique.
  • The user can choose between different types of pulse types. Each of these kinds is related to optimization of a given situation, such as lowered levels of spatter during welding.  
  • Pulsed arc welding techniques can either increase or decrease the welding productivity. It depends of the type of pulse that is selected.
  • Welding in is feasible in different types of positions

The development of different types of pulse arc techniques is significant. Consequently, the numbers of different pulse arc techniques increases in time.

Droplet transfer at pulse arc welding

The welding condition that is to be optimized determines if the pulse sequence will generate spray or short arc welding.  
Each droplet transfer is generated by one or several pulse sequences in a row, see the illustration below.

Example of current/time appearance during pulsed arc welding. This sequence illustrates a spray arc droplet transfer that is generated by each pulse.

Category and tags

How to weldShielding gas

Contact Technical support


The information in this report is only applicable to SSAB’s products and should not be applied to any other products than original SSAB products. 


This report provides general results and recommendations for SSAB steel products. This report is subject to SSAB’s Terms of Use. It shall be the user's responsibility to verify that the information contained herein is correct and is suitable to be used for the particular purpose and application of the user. The report is intended to be used by professional users only who possess adequate expertise, qualification and knowledge for the safe and correct use of the results and recommendations in this report. This report is provided “as is”. The use of the report is at user’s own discretion and risk and that users will be solely responsible for any use of this report. SSAB disclaims any liability for the content or potential errors of this report, including but not limited to warranties and condition of merchantability or fitness for a particular purpose or suitability for individual applications. SSAB shall not be liable for any kind of direct or indirect damages and/or costs related to or arising therefrom, whether special, incidental, consequential or directly or indirectly related to the use of, or the inability to use, the report or the content, information or results included therein.