Spray arc welding normally has a rather high heat input which leads to higher productivity compared to short arc welding.

This arc has a degree of stability that contributes to a very low level of spatter. Spray arc can be performed in the flat position.

Using rutile flux-cored wires gives the advantage of welding in positions other than the flat position.

The main welding positions, related to the position of the welding torch, according to the norm EN ISO 6947.

The high heat input means that the range of suitable single plate thicknesses for this technique is limited to approximately 5 mm and above. The exception is pulsed arc welding, which can weld joints of thinner single plate thicknesses. The sound from spray arc welding can be distinguished from short arc welding by its uniform character.

Droplet transfer at spray arc welding

The metal droplet transfer has a higher frequency compared to short arc welding and the size of each metal droplet is small. In spray arc welding there are no short circuits and the droplet leaves the wire as a small droplet or a spray through the arc, according to the illustration below.

MAG welding with a spray arc: a) Welding gun. b) Droplet. c) Base metal. d) Consumable electrode. e) Shielding gas. f) Weld pool.

Category and tags

How to weldShielding gas

Contact Technical support


The information in this report is only applicable to SSAB’s products and should not be applied to any other products than original SSAB products. 


This report provides general results and recommendations for SSAB steel products. This report is subject to SSAB’s Terms of Use. It shall be the user's responsibility to verify that the information contained herein is correct and is suitable to be used for the particular purpose and application of the user. The report is intended to be used by professional users only who possess adequate expertise, qualification and knowledge for the safe and correct use of the results and recommendations in this report. This report is provided “as is”. The use of the report is at user’s own discretion and risk and that users will be solely responsible for any use of this report. SSAB disclaims any liability for the content or potential errors of this report, including but not limited to warranties and condition of merchantability or fitness for a particular purpose or suitability for individual applications. SSAB shall not be liable for any kind of direct or indirect damages and/or costs related to or arising therefrom, whether special, incidental, consequential or directly or indirectly related to the use of, or the inability to use, the report or the content, information or results included therein. 

Copyright 2026