High reliability high versatility

SSAB Domex® comes as hot rolled plate, hot or cold rolled strip, tubes and sections. It’s also available in different metal-coated grades for corrosion resistance with zinc, galfan and galvannealed coatings.

Contact sales

    Hot rolled plate

    Hide/Show specific columns Edit
    Select columns to display
      Product Name Dimensions Standards Datasheet
      SSAB Domex 355ML T: 6.00 - 63.00 mm
      W: Up to 3300 mm
      EN 10025-4
      SSAB Domex 420ML T: 7.00 - 63.00 mm
      W: Up to 3300 mm
      EN 10025-4
      SSAB Domex 460ML T: 8.00 - 63.00 mm
      W: Up to 3300 mm
      EN 10025-4
      SSAB Domex 500ML T: 8.00 - 60.00 mm
      W: Up to 3300 mm
      SSAB
      Compare parameters

      Select one parameter to compare

      Comparison

        Hot rolled strip

        Hide/Show specific columns Edit
        Select columns to display
          Product Name Dimensions Standards Datasheet
          SSAB Domex 240YP T: 1.80 - 20.00 mm
          W: Up to 1860 mm
          EN 10025-2
          SSAB Domex 315MC T: 1.80 - 18.00 mm
          W: Up to 1860 mm
          EN 10149-2
          SSAB Domex 355MC T: 1.80 - 16.00 mm
          W: Up to 1860 mm
          EN 10149-2
          SSAB Domex 420MC T: 1.80 - 15.00 mm
          W: Up to 1800 mm
          EN 10149-2
          SSAB Domex 460MC T: 2.00 - 13.00 mm
          W: Up to 1800 mm
          EN 10149-2
          SSAB Domex 500MC T: 2.00 - 13.00 mm
          W: Up to 1800 mm
          EN 10149-2
          SSAB Domex 550MC T: 2.00 - 12.80 mm
          W: Up to 1640 mm
          EN 10149-2
          SSAB Domex 355MC Plus T: 3.00 - 12.00 mm
          W: Up to 1860 mm
          EN 10149-2
          SSAB Domex 420MC Plus T: 3.00 - 10.00 mm
          W: Up to 1860 mm
          EN 10149-2
          SSAB Domex 460MC Plus T: 4.00 - 10.00 mm
          W: Up to 1800 mm
          EN 10149-2
          SSAB Domex 500MC Plus T: 3.00 - 8.00 mm
          W: Up to 1800 mm
          EN 10149-2
          Compare parameters

          Select one parameter to compare

          Comparison

            Cold rolled strip

            Hide/Show specific columns Edit
            Select columns to display
              Product Name Dimensions Standards Datasheet
              SSAB Domex® 220LA T: 0.40 - 3.00 mm
              W: Up to 1500 mm
              SSAB
              SSAB Domex® 260LA T: 0.50 - 3.00 mm
              W: Up to 1500 mm
              EN 10268
              SSAB Domex® 280LA T: 0.40 - 3.00 mm
              W: Up to 1500 mm
              SSAB
              SSAB Domex® 300LA T: 0.40 - 3.00 mm
              W: Up to 1500 mm
              EN 10268
              SSAB Domex® 340LA T: 0.40 - 3.00 mm
              W: Up to 1500 mm
              EN 10268
              SSAB Domex® 350LA T: 0.45 - 3.00 mm
              W: Up to 1500 mm
              SSAB
              SSAB Domex® 380LA T: 0.45 - 3.00 mm
              W: Up to 1500 mm
              EN 10268
              SSAB Domex® 420LA T: 0.50 - 3.00 mm
              W: Up to 1500 mm
              EN 10268
              SSAB Domex® 460LA T: 0.50 - 1.60 mm
              W: Up to 1500 mm
              EN 10268
              SSAB Domex® 500LA T: 0.45 - 3.00 mm
              W: Up to 1500 mm
              EN 10268
              Compare parameters

              Select one parameter to compare

              Comparison

                Metal-coated strip

                Hide/Show specific columns Edit
                Select columns to display
                  Product Name Dimensions Standards Datasheet
                  SSAB Domex® 220LAD T: 0.50 - 3.00 mm
                  W: Up to 1520 mm
                  SSAB
                  SSAB Domex® 260LAD T: 0.50 - 3.00 mm
                  W: Up to 1520 mm
                  EN 10346
                  SSAB Domex® 300LAD T: 0.50 - 3.00 mm
                  W: Up to 1520 mm
                  EN 10346
                  SSAB Domex® 340LAD T: 0.50 - 3.00 mm
                  W: Up to 1520 mm
                  EN 10346
                  SSAB Domex® 380LAD T: 0.50 - 3.00 mm
                  W: Up to 1520 mm
                  EN 10346
                  SSAB Domex® 420LAD T: 0.50 - 3.00 mm
                  W: Up to 1520 mm
                  EN 10346
                  SSAB Domex® 460LAD T: 0.80 - 3.00 mm
                  W: Up to 1500 mm
                  EN 10346
                  SSAB Domex® 500LAD T: 0.80 - 2.00 mm
                  W: Up to 1410 mm
                  EN 10346
                  SSAB Domex® 220GD T: 0.45 - 3.00 mm
                  W: Up to 1520 mm
                  EN 10346
                  SSAB Domex® 250GD T: 0.45 - 3.00 mm
                  W: Up to 1520 mm
                  EN 10346
                  SSAB Domex® 280GD T: 0.45 - 3.00 mm
                  W: Up to 1520 mm
                  EN 10346
                  SSAB Domex® 320GD T: 0.50 - 3.00 mm
                  W: Up to 1520 mm
                  EN 10346
                  SSAB Domex® 350GD T: 0.50 - 3.00 mm
                  W: Up to 1520 mm
                  EN 10346
                  Compare parameters

                  Select one parameter to compare

                  Comparison

                    Tubes and sections

                    Hide/Show specific columns Edit
                    Select columns to display
                      Product Name Dimensions Standards Datasheet
                      SSAB Domex Tube 460MH Circular: 42.4 - 323.9 mm
                      Square: 40x40 - 300x300 mm
                      Rectangular: 50x30 - 400x200 mm
                      Wall Thickness: 2.0 - 12.5 mm
                      EN 10219-1, EN 10219-2
                      SSAB Domex Tube 500MH Circular: 42.4 - 323.9 mm
                      Square: 40x40 - 300x300 mm
                      Rectangular: 50x30 - 400x200 mm
                      Wall Thickness: 2.0 - 12.5 mm
                      EN 10219-2, EN 1090-2
                      SSAB Domex Tube 550MH Circular: 42.4 - 323.9 mm
                      Square: 40x40 - 300x300 mm
                      Rectangular: 50x30 - 400x200 mm
                      Wall Thickness: 2.0 - 12.50 mm
                      EN 10219-2, EN 1090-2
                      SSAB Domex Tube Double Grade Circular: 42.4 - 323.9 mm
                      Square: 40x40 - 300x300 mm
                      Rectangular: 50x30 - 400x200 mm
                      Wall Thickness: 2.0 - 12.50 mm
                      EN 10219-1, EN 10219-2
                      Circular: 42.4 - 323.9 mm
                      Square: 40x40 - 300x300 mm
                      Rectangular: 50x30 - 400x200 mm
                      Wall Thickness: 2.0 - 12.50 mm
                      EN 10219-1, EN 10219-2
                      SSAB Domex Tube 235 JRH Circular: 42.4 - 323.9 mm
                      Square: 40x40 - 300x300 mm
                      Rectangular: 50x30 - 400x200 mm
                      Wall Thickness: 2.0 - 12.50 mm
                      EN 10219-1, EN 10219-2
                      SSAB Domex Tube 355J2H Circular: 42.4 - 323.9 mm
                      Square: 40x40 - 300x300 mm
                      Rectangular: 50x30 - 400x200 mm
                      Wall Thickness: 2.0 - 12.5 mm
                      EN 10219-1, EN 10219-2
                      Compare parameters

                      Select one parameter to compare

                      Comparison

                        180