Wear design > Wear > Lining guidelines for mining truck bodies

Carryback

Ore or overburden can become very sticky after rainfall or when materials are at risk of freezing. Sharp corners tend to accumulate this sticky material, and the relatively low flow in these corners makes it difficult for the material to wear off. To address this issue, the corners can be redesigned with a larger radius to improve flow and reduce material buildup.

Carryback at the bottom and sides of a mining truck body. The problem is solved by rounding the corners.

Category and tags

Wear designWear

Contact Technical support


The information in this report is only applicable to SSAB’s products and should not be applied to any other products than original SSAB products. 


This report provides general results and recommendations for SSAB steel products. This report is subject to SSAB’s Terms of Use. It shall be the user's responsibility to verify that the information contained herein is correct and is suitable to be used for the particular purpose and application of the user. The report is intended to be used by professional users only who possess adequate expertise, qualification and knowledge for the safe and correct use of the results and recommendations in this report. This report is provided “as is”. The use of the report is at user’s own discretion and risk and that users will be solely responsible for any use of this report. SSAB disclaims any liability for the content or potential errors of this report, including but not limited to warranties and condition of merchantability or fitness for a particular purpose or suitability for individual applications. SSAB shall not be liable for any kind of direct or indirect damages and/or costs related to or arising therefrom, whether special, incidental, consequential or directly or indirectly related to the use of, or the inability to use, the report or the content, information or results included therein. 

Copyright 2026