SSAB´s comprehensive range of cold-formed open steel sections includes extremely varied possibilities for both steel grades (up to S900) and shapes. A steel and shape exactly matching the application provides significant weight and cost savings. Each unit of weight saved will offer direct benefits in transportation and in the lighter weight of structures. Our cold-formed open sections are made according to EN 10162.
In addition to standard section shapes, we can also deliver sections tailored to your specific needs using the most suitable materials for the application. Tailoring section properties to your needs can give your end product a significant competitive edge and boost your production efficiency.
The choice of steel section shapes is endless. We can produce thousands of different shapes, delivered laser cut, sand blasted, painted, hot-dip galvanized or zinc coated. Material is available up to 12.5 mm thickness in lengths varying from 0.4 m to 21 m.
SSAB’s cold-formed steel sections are suitable for practically any kind of steel structure, whether for commercial or residential buildings, machines or appliances.
The accuracy of the cross-sectional form and good formability for high-strength material makes it possible to create long-lasting and light structures.
Typical applications are frames and sub-frames, vehicle and trailer bodies, warehouse equipment and masts.
This U-section series has been developed with same outside dimensions as UNP-beams so that replacing hot-rolled beams is easier. Thickness is selected so that cold-formed U-section has the same bending strength but it weighs less. Weight saving has been achieved by using higher strength steel grade.
Cold-formed U-sections S355MC | Hot-rolled UNP-beams S235JR EN 10025-2 | ||||||||||
h/b | t | M | NR1) | VR2) | MR3) | MR3) | VR2) | NR1) | M | UNP | |
mm/mm | mm | kg/m | kN | kN | kNm | kNm | kN | kN | kg/m | ||
50/38 | 5 | 4.27 | 193 | 43.8 | 2.82 | 2.49 | 25.4* | 167 | 5.59 | 50 | |
65/42 | 5 | 5.17 | 234 | 57.6 | 4.5 | 4.16 | 38.8* | 212 | 7.09 | 65 | |
80/45 | 5 | 6 | 271 | 71.2 | 6.4 | 6.23 | 56.4 | 259 | 8.64 | 80 | |
100/50 | 5 | 7.17 | 324 | 89.3 | 9.55 | 9.68 | 71.1 | 317 | 10.6 | 100 | |
120/55 | 6 | 9.91 | 448 | 127.6 | 15.48 | 14.3 | 99 | 400 | 13.4 | 120 | |
140/60 | 6 | 11.32 | 512 | 149.2 | 20.61 | 20.3 | 116 | 479 | 16 | 140 | |
160/65 | 6 | 12.73 | 576 | 170.7 | 26.45 | 27.3 | 142 | 564 | 18.8 | 160 | |
180/70 | 7 | 16.37 | 740 | 222.8 | 37.71 | 35.3 | 170 | 658 | 22 | 180 | |
200/75 | 7 | 18.02 | 815 | 247.8 | 46.1 | 44.9 | 201 | 757 | 25.3 | 200 | |
220/80 | 8 | 22.22 | 1005 | 309.7 | 61.59 | 57.6 | 234 | 879 | 29.4 | 220 | |
240/85 | 8 | 24.1 | 1090 | 338.2 | 72.92 | 70.5 | 269 | 994 | 33.2 | 240 | |
260/90 | 8 | 25.98 | 1175 | 366.7 | 85.2 | 87.2 | 308 | 1135 | 37.9 | 260 | |
280/95 | 9 | 31.18 | 1410 | 442.8 | 109.2 | 105 | 333 | 1253 | 41.8 | 280 | |
300/100 | 9 | 33.3 | 1506 | 474.8 | 125.03 | 126 | 358 | 1382 | 46.2 | 300 | |
320/100 | 11 | 41.71 | 1886 | 610.3 | 161.29 | 160 | 520 | 1781 | 59.5 | 320 | |
350/100 | 10.5 | 42.53 | 1923 | 635.1 | 177.71 | 172 | 552 | 1817 | 60.6 | 350 | |
400/110 | 11.5 | 52.53 | 2375 | 792.5 | 248.54 | 240 | 650 | 2150 | 71.8 | 400 |