SSAB AM Agile

Download data sheet

General Product Description

SSAB AM Agile is a gas atomized low-alloyed powder for additive manufacturing of high strength components and tooling applications. The spherical powder is in particular suited for L-PBF (Laser Powder Bed Fusion) and DED (Direct Energy Deposition).

The printed components have a great combination of strength, toughness and hardness in as-printed condition (without additional heat treatment). The as-printed properties give a versatile use such as high-performance components for light weight constructions and engineering products. The as-printed properties also give excellent thermal conductivity and polishability for tooling inserts. The mechanical properties of SSAB AM Agile can by modified through additional heat treatment.

SSAB AM Agile is a steel grade with low CO2 emissions, available as SSAB Zero™. SSAB AM Agile is also planned for fossil-free properties (see www.ssab.com/fossilfree).

Powder Properties

Standard particle size distribution.

L-PBF

20 - 53 µm

DED

53 - 150 µm

Measurement of particle size distribution is according to ISO 13322-2 (Dynamic image analysis methods).

Other particle size distributions can be arranged upon agreement.

Generic Data

Achievable generic data in as-built parts: L-PBF

Density

7.8 g/cm3

Young´s Modulus

200 GPa

 

Physical Properties

+20 °C
Heat conductivity (W/m*K)
24
Thermal expansion coefficient (10-6/K)
13
+200 °C
Heat conductivity (W/m*K)
29
Thermal expansion coefficient (10-6/K)
14
+400 °C
Heat conductivity (W/m*K)
32
Thermal expansion coefficient (10-6/K)
14

 

Mechanical Properties

Achievable mechanical properties in as-built parts: L-PBF

Product
Product
SSAB AM Agile
Hardness
(HV5)
450
Tensile strength
(MPa)
1370
Yield strength
(MPa)
1210
Elongation A5
(%)
14
Impact toughness
(Charpy V)
at RT 1)/ at -40 oC
70 J / 40 J

1) At room temperature.

All test samples have been produced on a SLM 280 2.0 system, 30 µm layer thickness and tested in the vertical direction.

Typical Chemical Composition

C
(%)
C
(%)
0.30
Si
(%)
1.06
Mn
(%)
0.75
Cr
(%)
1.38
Mo
(%)
0.77
Ni
(%)
0.70
V
(%)
0.14
Fe
Balance

 

Delivery Conditions

Standard package size for SSAB AM powder is 10 kg, including silica gel bag. Other package sizes are available up on agreement.

 

Safety Information Sheet

SSAB Zero™

SSAB Zero™ is made of recycled steel and produced with fossil-free electricity and biogas. It has virtually no fossil carbon emissions during steel production, without mass balancing allocation of emission reduction or carbon emission offsetting. SSAB Zero™ has the same quality and properties as the traditional steel versions. More details are given in SSAB Zero™ Certificate of Carbon Emissions at www.ssab.com.