Farmtech’s agricultural tippers made from Hardox® steel are “indestructible,” according to customers

In the midst of the beautiful Slovenian countryside, tipper body specialist Farmtech constructs high-quality equipment for the demanding agricultural industry, which runs continuous transports with heavy loads. The recipe for the success of the heavy-duty dump tipper Gravis 2000 is to use Hardox® 450 wear plate throughout the model’s body.

The conical shape of Farmtech’s Gravis 2000 dumper body is made exclusively out of Hardox® 450 wear plate. This ensures endurance during the hard work of the agricultural industry, transporting dirt and big rocks, both off-road and on-road.

Farmtech is situated in the vicinity of Ljutomer in the dead center of Slovenian farmland, with fields stretching all around as far as the eye can see. Wanting the equipment to last longer, the farmers, hauling not only grain but also heavy soil and rocks, need the highest level of quality for their agricultural machinery.

“We have been using Hardox steel for many years, so we knew that it would be the perfect fit for the Gravis 2000,” says Miro Hajdinjak, development manager at Farmtech. “We decided to design the tipper body entirely out of Hardox 450, which gave an extra advantage.”

The most critical part is the floor, which is subject to very big loads. But the sides of the tipper body also need to withstand a lot of wear and tear.

“We have been using Hardox steel for many years, so we knew that it would be the perfect fit for the Gravis 2000.”

Miro Hajdinjak, development manager at Farmtech


Hardox® steel meets all demands

“Hardox is a material that corresponds to all our needs,” Hajdinjak explains. “Having Hardox in our tippers means we can use a thinner wear plate because it is stronger than other steel materials. A thinner, yet stronger steel, means that we can reduce the weight of the tipper, so our end customers can increase the load that they transport from point A to point B. This is why all our customers are happy with the product.”

Road regulations specify a maximum weight for vehicles. So, when carrying heavy material, the more the tipper can carry, the fewer trips it needs to make. Even with a payload of 26 tons, the end customer complies with the vehicle weight regulations, reducing fuel consumption. The productivity of Gravis 2000 is also boosted by the longer life span that Hardox® steel offer.

“Hardox 450 ensures durability of the tipper trailer,” Hajdinjak says. “Buying a trailer with a body made of Hardox has many advantages. The life span is longer due to less wear and tear, and there is a bigger marketability because of the customer knowledge of the material.”


Hardox® In My Body is a guarantee of quality

Being a Hardox® In My Body customer program member gives Farmtech an advantage in the market, as it is a guarantee for customers that the dump tippers are made out of high-quality steel. This is something Franz Jantscher, operational manager at Farmtech, has firsthand experience with. He knows that the customers need to be able to rely on the quality of the agricultural equipment.

“We get very good feedback from our customers,” Jantscher says. “They say it’s not cheap, but it's indestructible. Compared to our competitors, our vehicles offer a much higher stability and wear resistance.”

Jantscher explains that the Hardox® In My Body sign is very well known and much appreciated by customers. Farmtech serves a market all over Europe. Most of its customers are in Germany, Switzerland and Austria, but there are others in Slovenia, Croatia, Serbia and Hungary.

“It is an advantage for us if we can demonstrate that we are using Hardox, which means that we are using a high-strength material,” he says. “Reliability and wear resistance are playing an important role, and the Hardox In My Body sign makes it possible for our customers to trust our products.”

About Farmtech

  • Austrian-owned agricultural equipment company with factory facilities in Ljutomer, Slovenia
  • Dedicated to farming equipment for over 50 years
  • Part of Komptech Group and one of the leading agricultural machine companies in Europe
  • Core markets: Austria, Croatia, Germany, Hungary, Serbia, Slovenia and Switzerland

www.farmtech.eu

 

SSAB steel used in Farmtech’s products

  • Hardox® 450 wear plate throughout the body of the Gravis 2000 agricultural dump tipper
    • 8-millimeter thickness in the floor
    • 6-millimeter thickness in the walls
  • Hardox® steel is also used in other parts that are subject to wear and tear, such as trailer parts and knives in spreaders

Contact us

No matter where you are located, we have local support that can answer your questions.

Sign up for newsletters

Visit our subscription center to manage all your SSAB newsletters subscriptions

Don't miss out!

Hardox® wear plate

Hardox® wear plate is the world's leading abrasion-resistant (AR) steel. Hardox® is hard through and through, from the surface deep down to its core, giving you extended service life and high productivity in the most challenging environments.

Hardox® In My Body

Look for the Hardox® In My Body branded sign if you’re looking for bodies that are hard, tough, cost efficient and made from genuine Hardox® wear plate.

Related articles

Mar 25 2020

Betonstar reaches higher with lighter weight through Strenx® steel

Concrete pumps used in the construction of tall buildings need a boom structure that is strong and reliable while also striving for light weight. Turkish Betonstar has met these requirements by using only Strenx® performance steel throughout its structures. The result is longer, stronger and lighter products.

Feb 25 2020

By incorporating Hardox® and Strenx® steels in tippers, Fesan makes sure not to compromise on quality

Turkish trailer and tipper manufacturer Fesan Makina’s key driver is customer satisfaction. When customers asked for stronger and lighter equipment, that is what they got, as Fesan switched to Hardox® wear plate and Strenx® performance steel. By including this and other innovative features in the new tipper model, the company is keeping its position as a market leader.

Jan 29 2020

AA Diesel Truck Bodies gains 10-plus years of product life for end users with Hardox® wear plate

For 20 years, family company AA Diesel Truck Bodies has supplied custom-made truck bodies to the demanding Australian transport industry. The right steel in the body units will help the end user to reduce weight by 10 to 20 percent and increase the payload.

180