How to weld > Welding on primed steel

Suitable welding performances

Welding can be performed with or without leaving the primer in the joint.

When the primer is left on it is possible to attain advantageous results of the general properties in the joint. It is also feasible to perform welding with the same parameters as for welding a joint without a primer. However, the outcome may be further improved if the primer is removed from the joint and the adjacent surroundings prior to welding.

If the primer is left on in the joint, MAG-welding with basic types of flux cored wires is a good option since it supports a lowered level of porosity. However, beneficially low porosity levels in the weld metal can be attained in general for all other types of welding methods welded with the recommended consumables.

Contact Technical support


The information in this report is only applicable to SSAB’s products and should not be applied to any other products than original SSAB products. 


This report provides general results and recommendations for SSAB steel products. This report is subject to SSAB’s Terms of Use. It shall be the user's responsibility to verify that the information contained herein is correct and is suitable to be used for the particular purpose and application of the user. The report is intended to be used by professional users only who possess adequate expertise, qualification and knowledge for the safe and correct use of the results and recommendations in this report. This report is provided “as is”. The use of the report is at user’s own discretion and risk and that users will be solely responsible for any use of this report. SSAB disclaims any liability for the content or potential errors of this report, including but not limited to warranties and condition of merchantability or fitness for a particular purpose or suitability for individual applications. SSAB shall not be liable for any kind of direct or indirect damages and/or costs related to or arising therefrom, whether special, incidental, consequential or directly or indirectly related to the use of, or the inability to use, the report or the content, information or results included therein. 